Abstract
The pinning field in an MR device was significantly improved by using the Ru 4A peak together with steps to minimize interfacial roughness of the ruthenium layer as well as boron and manganese diffusion into the ruthenium layer during manufacturing. This made it possible to anneal at temperatures as high as 340° C. whereby a high MR ratio could be simultaneously achieved.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method to provide a tunneling magneto resistive (TMR) device with both a high internal pinning strength as well as with a high magneto-resistive (MR) ratio, comprising: prior to annealing said TMR device, reducing interfacial roughness of a ruthenium layer located between said TMR's first anti-parallel (AP1) layer and said TMR's second anti-parallel (AP2 ) layer; minimizing boron diffusion from said AP1 layer into said ruthenium layer; and minimizing manganese diffusion from a layer of antiferromagnetic (AFM) material into said ruthenium layer.
- Claim 2Depends on #1
The method described in claim 1 wherein said TMR device has both a TMR ratio of at least 50% as well as an internal pinning strength of at least 5,000 Oe.
- Claim 3Depends on #1
The method described in claim 1 wherein said ruthenium layer has a thickness between 3 and 4.5 Angstroms whereby it is optim