Nano-oxide based current-perpendicular-to-plane (CPP) magnetoresistive (MR) sensor stacks are provided, together with methods for forming such stacks. Such stacks have increased resistance and enhanced magnetoresistive properties relative to CPP stacks made entirely of metallic…
Headway Technologies Inc
A method for the detection of magnetic beads at temperature below room temperature can increase the signal level significantly as compared to the same detection when performed at room temperature. Additional improvement is obtained if the beads are below 30nm in size and if…
PROBLEM TO BE SOLVED: To provide a magnetoresistance sensor element of a spin bubble type, where reading of magnetic recording information of ultrahigh density of 20 Gb/in2 in higher is enabled, and a manufacturing method of the sensor element. SOLUTION: A lower base substance…
<P>PROBLEM TO BE SOLVED: To provide a CPP-GMR (current perpendicular to plane-giant magneto-resistive effect) reproducing head capable of improving reproducing performance in a stable manner. <P>SOLUTION: An anti-parallel ferromagnetic layer (AP1) 15 located on the…
<P>PROBLEM TO BE SOLVED: To provide a magnetic head capable of increasing a protrusion amount of a playback head structure. <P>SOLUTION: In the magnetic head including a playback head structure 100 and a recording head structure 200, a lower playback shield layer 4…
<P>PROBLEM TO BE SOLVED: To provide a perpendicular magnetic recording head reducing a side fringe magnetic field while maintaining sufficient magnetic field intensity. <P>SOLUTION: The PMR head 30 includes, on a base body 31, a narrow width part 351 of a main…
A magnetic head includes a main pole, a trailing shield, a spin torque oscillator, and a buffer layer. The buffer layer is interposed between the main pole and the spin torque oscillator. The spin torque oscillator has first and second side surfaces. The first and second side…
A method for forming a planar GMR read-head having a narrow read gap, a narrow track-width and being well insulated from its lower shield. The method requires the formation of a planarized bottom magnetic shield in which concave regions, symmetrically disposed about a…
Currently, the shield-to-shield separation of a spin valve head cannot be below about 800 Å, mainly due to sensor-to-lead shorting problems. This problem has now been overcome by inserting a high permeability, high resistivity, thin film shield on the top or bottom (or both)…
A CPP-GMR spin value sensor structure with an improved MR ratio and increased resistance is disclosed. All layers except certain pinned layers, copper spacers, and a Ta capping layer are oxygen doped by adding a partial O 2 pressure to the Ar sputtering gas during deposition.…
An MTJ is disclosed in which the free layer and reference layer have a vortex magnetization state that is formed with a clockwise or counterclockwise rotation. The MTJ has a low aspect ratio elliptical shape and the magnetic layers have a dopant that is one of C, N, B, Zr, Ta,…
The present invention has a configuration which allows manufacturing a capacitor comprising a first electrode layer, conductive first convex sections layered on a surface of the first electrode layer, a first dielectric layer formed on a surface of the first convex sections and…
A main pole layer is deposited within an opening in a patterned photoresist layer on a substrate. The photoresist is thinned to expose an upper portion of a pole tip region that is then trimmed to a rectangular shape while a lower portion retains an inverted trapezoidal shape.…
A near-field light generating element has an outer surface. The outer surface includes a bottom surface, first and second inclined surfaces, an edge part that connects the first and second inclined surfaces to each other, and a front end face located in a medium facing surface.…
A high performance TMR sensor is fabricated by employing a free layer with a trilayer configurations represented by FeCo/CoFeB/CoB, FeCo/CoB/CoFeB, FeCo/CoFe/CoB, or FeCo/FeB/CoB may also be employed. Alternatively, CoNiFeB or CoNiFeBM formed by co-sputtering CoB with CoNiFe or…
A layered chip package includes a main body and wiring. The main body includes a main part including a plurality of stacked layer portions, and a plurality of terminals disposed on the top and bottom surfaces of the main part. The wiring includes a plurality of lines…
A magnetic head includes a coil, a main pole, a write shield, and first and second yoke layers. The first and second yoke layers are magnetically connected to the write shield and aligned along the direction of travel of a recording medium such that the main pole is interposed…
A PMR writer is disclosed wherein a magnetic assist layer (MAL) made of an anisotropic (−Ku) or (+Ku) magnetic material is formed along a main pole trailing side to optimize the vertical magnetic field and field gradient at the air bearing surface. A Ru seed layer is formed…
A TAMR (Thermal Assisted Magnetic Recording) writer has a narrow pole tip with a trailing edge magnetic shield. The narrow pole tipped write head uses the energy of laser generated edge plasmons, formed in a plasmon generating layer, to locally heat a PMR magnetic recording…
The possibility of shorting between a spin valve and its underlying magnetic shield layer can be largely eliminated by choosing the bottom spin valve structure. However, doing so causes the hard longitudinal bias that is standard for all such devices to degrade. The present…
A composite layered chip package includes a plurality of subpackages stacked. Each subpackage includes a main body, and wiring disposed on a side surface of the main body. The main body has a main part that includes at least one first-type layer portion. For any two vertically…
A CPP-GMR spin valve having a composite spacer layer comprised of at least one metal (M) layer and at least one semiconductor or semi-metal (S) layer is disclosed. The composite spacer may have a M/S, S/M, M/S/M, S/M/S, M/S/M/S/M, or a multilayer (M/S/M) n configuration where n…
A CPP-GMR spin valve having a CoFe/NiFe composite free layer is disclosed in which Fe content of the CoFe layer ranges from 20 to 70 atomic % and Ni content in the NiFe layer varies, from 85 to 100 atomic % to maintain low Hc and λ s values. A small positive magnetostriction…
As track densities increase, it becomes increasingly important, while writing in a given track, not to inadvertently write data in adjoining tracks. This problem has been overcome by limiting the width of material in the ABS plane to what it is at the write gap. The part of the…