US 8,307,688 B2#105008693 Most CitedActiveUnited States (USPTO)Utility

Process for producing seamless stainless steel pipe

0Forward Citations (#105008693 Global)
0.0/yrCitation Velocity (#105008693 Global)
0.56Citation PageRank (#105008693 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing seamless pipes which comprises conducting a piercing rolling step, a elongating rolling step using a mandrel bar, and a sizing rolling step and subsequently conducting a product heat treatment. In the process, when the carbon-equivalent weight, namely the sum of the weight of graphite in the lubricant and the carbon content in the organic binder, per unit area of the lubricant adhering to the mandrel bar surface in the above-mentioned step of elongating rolling is expressed by C (g/m 2 ) or the maximum extent of carburization in the inner surface of the pipe to be heat-treated but prior to the heat treatment is expressed by ΔC (% by mass), the heating temperature for the pipe to be heat-treated is expressed by T (° C.), and the time during which a decarburizing gas is blown into the inside of the pipe to be heat-treated is expressed by t 1 or t 2 (seconds), and further, the blowing time calculated taking into account the wall thickness reduction in the step of cold working is expressed by t 3 or t 4 (seconds), a predetermined relation is satisfied and the actual decarburizing gas blowing time in the heat treatment is longer than the time t 1 , t 2 , t 3 or t

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing seamless stainless steel pipes in which the process includes the steps of: piercing rolling; elongating rolling using a mandrel bar; and sizing rolling, followed by a product heat treatment, wherein when the carbon-equivalent weight, which is the sum of the weight of graphite in and the weight of the carbon content of organic binder in a lubricant used for the mandrel bar, per unit area of the lubricant adhering to the mandrel bar surface in the above-mentioned step of elongating rolling, is C (g/m 2 ), and a heating temperature for the pipe to be heat-treated in the ab

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (5)

  • International Preliminary Examination Report from corresponding PCT/JP2007/060391 dated Aug. 21, 2007. (Japanese language only).
  • International Search Report from corresponding PCT/JP2007/060391 dated Aug. 21, 2007.
  • Translation-International Preliminary Report on Patentability from corresponding PCT/JP2007/060391, 3 pages.
  • Translation—International Preliminary Report on Patentability from corresponding PCT/JP2007/060391, 3 pages.
  • Written Opinion from corresponding PCT/JP2007/060391 dated Aug. 21, 2007. (Japanese language only).