Patents
Assignee / Organization

Iida Sumio

65Total Forward Citations
31Indexed Patents
2Avg Citations / Patent
5Portfolio H-Index
WO 2004/108311 A1#12956512 Most Cited · 8 citations0.4/yr · PR 2.15PendingWO · Application
Cr-PLATED MADNREL BAR FOR MANUFACTURING HOT SEAMLESS TUBE AND METHOD OF MANUFACTURING THE SAME

A Cr-plated mandrel bar for manufacturing a hot seamless tube and a method of manufacturing the mandrel bar, the mandrel bar wherein since the maximum depths (Rv) thereof in the axial and circumferential directions are specified together with average centerline roughnesses (Ra)…

WO 2006/054768 A1#17866291 Most Cited · 6 citations0.3/yr · PR 1.58PendingWO · Application
Powder lubricant composition for hot working and process for producing seamless tube

A powder lubricant composition for hot working which comprises sodium borate in an anhydrous, pentahydrate, or decahydrate form and the sodium salt or calcium salt of a fatty acid and further contains calcium carbonate or lithium carbonate as a lubricant aid. Due to the…

WO 2007/122972 A1#16867032 Most Cited · 6 citations0.3/yr · PR 2.01PendingWO · Application
Lubricant composition for hot plastic working and method of hot plastic working with the same

A lubricant composition for hot plastic working and a method of hot plastic working which are effective in preventing the surface of a material being processed by hot plastic working from suffering mars. The lubricant composition for hot plastic working is characterized by…

US 2008083254 A1#21553811 Most Cited · 5 citations0.3/yr · PR 1.37PendingUS · Application
Manufacturing method and cleaning equipment for seamless tube

A seamless tube is manufactured while effectively suppressing the occurrence of carburization in the seamless tube without interfering with operations. A seamless tube is manufactured by a step of washing at least a portion of a conveyor installed in a conveying step of a…

US 2009054279 A1#19134026 Most Cited · 5 citations0.3/yr · PR 2.82PendingUS · Application
Two-Component Anti-Seizure Agent for Hot Metal Working Process, and Method of Manufacturing Seamless Pipe Using Thereof

The present invention provide a two-component anti-seizure agent for hot metal working process comprising the first aqueous solution and the second aqueous solution, wherein the first aqueous solution contains 10˜30 mass % of sodium silicate equivalent to anhydride to 100 mass %…

US 2007157691 A1#25578504 Most Cited · 4 citations0.2/yr · PR 1.29PendingUS · Application
Process for producing seamless steel pipe
Inventors: Iida Sumio, Nakanishi TetsuyaAssignee: Iida Sumio, Nakanishi TetsuyaFiled 2006-12-15

A process for producing a seamless steel pipe, in which the occurrence of inner surface flaws in the pipe can be reduced through the lowering of the friction coefficient during the elongation rolling by means of a mandrel mill is provided. The reduction of inner surface flaws is…

WO 2006/106961 A1#24077142 Most Cited · 4 citations0.2/yr · PR 1.49PendingWO · Application
Process for producing seamless tube

A process which comprises: a first coating step in which a first liquid is applied to the surface of a high-temperature mandrel bar immediately after preceding stretching/rolling to thereby form a water-resistant coating film; a water-cooling step in which the mandrel bar which…

WO 2007/126005 A1#24845356 Most Cited · 4 citations0.2/yr · PR 1.37PendingWO · Application
Process for producing stainless-steel pipe

A process for stainless-steel pipe production which comprises piercing and rolling a stainless steel containing 10-30 mass% chromium as a raw material to obtain a raw pipe to be finish-rolled, rolling the raw pipe by drawing rolling with a mandrel using a graphite-free…

WO 2009/088036 A1#23390452 Most Cited · 4 citations0.2/yr · PR 1.70PendingWO · Application
Lubricant for hot working and process for manufacturing seamless steel pipe
Inventors: Saito Kenichi, Iida SumioAssignee: Sumitomo Metal Ind, Saito KenichiFiled 2009-01-08

A lubricant for hot plastic working which contains 20 to 40 mass% of iron oxide and 10 to 30mass% of sodium silicate and has an impurity content of 3mass% or below and which further contains 40 to 60mass% of water. The lubricant exhibits excellent lubricity and supply…

WO 2005/123289 A1#29320583 Most Cited · 3 citations0.1/yr · PR 1.33PendingWO · Application
Process for producing seamless steel pipe
Inventors: Iida Sumio, Nakanishi TetsuyaAssignee: Sumitomo Metal Ind, Iida SumioFiled 2005-06-15

A process for producing a seamless steel pipe, in which the occurrence of inner surface flaw in the pipe can be reduced through lowering of the friction coefficient at draw rolling by means of a mandrel mill. At the draw rolling of hollow stock pipe, a lubricant composed mainly…

US 2007287642 A1#35439087 Most Cited · 2 citations0.1/yr · PR 1.33PendingUS · Application
Powdered lubricant composition for hot working and method for manufacturing seamless tubes

With a powdered lubricant composition by the invention, in addition to the blending of one of anhydrous, pentahydrate or decahydrate salt in sodium borate and one of sodium or calcium salt of fat acid, mixing calcium or lithium carbonate as an auxiliary lubricant can prevent…

WO 2005/056740 A1#38693873 Most Cited · 2 citations0.1/yr · PR 1.05PendingWO · Application
Lubricant composition for hot forming

Disclosed is a lubricant composition for hot forming which contains 10-40 mass% of a solid lubricant, 5-20 mass% of a water-dispersible synthetic resin, 0.5-5 mass% of an amine salt of an inorganic acid, and 45-80 mass% of water. Such a lubricant composition for hot forming…

WO 2006/090718 A1#37270228 Most Cited · 2 citations0.1/yr · PR 1.12PendingWO · Application
Process for producing seamless pipe and cleaning equipment

This invention provides a process for producing a seamless pipe while effectively suppressing carburizing which occurs in a seamless pipe without affecting the operation. The production process comprises the steps of cleaning a transfer device disposed between a lubricant…

WO 2007/116653 A1#43096750 Most Cited · 2 citations0.1/yr · PR 0.94PendingWO · Application
Lubricant for hot plastic working and powder lubricant composition for hot working

The invention provides a lubricant for hot plastic working which can protect the surface of a workpiece from build-up of white scales due to a lubricant and which is improved in lubricating performance and can give finished products excellent in surface appearance. A lubricant…

WO 2008/023563 A1#36463905 Most Cited · 2 citations0.1/yr · PR 1.17PendingWO · Application
Mandrel bar cleaning facility

A mandrel bar cleaning facility in which carburizing occurring on the inner surface of a pipe during elongation can be suppressed without causing any trouble to operation. The mandrel bar cleaning facility (15) cleans a mandrel bar (B) drawn out from a mandrel bar carrying line…

WO 2005/023966 A1#46481180 Most Cited · 1 citations0.1/yr · PR 1.18PendingWO · Application
Lubricant composition for seamless steel pipe working
Inventors: Tanaka Kazuo, Mori Shizuo, Iida SumioAssignee: Sumitomo Metal Ind, Tanaka KazuoFiled 2004-09-03

A lubricant composition for seamless steel pipe working that without detriment to non-carburization properties and surpassing lubricity for hard-to-work materials such as 13-chrome steel and stainless steel, comprehensively satisfies requirements for properties such as storage…

WO 2006/008804 A1#47496064 Most Cited · 1 citations0.1/yr · PR 0.96PendingWO · Application
METHOD FOR HOT WORKING OF Cr-CONTAINING STEEL

A method for the hot working of a Cr-containing steel, which comprises holding a newly formed surface of the Cr-containing steel in a steam atmosphere, to thereby form an oxidized scale containing FeO, and then carrying out a subsequent hot working. More specifically, a method…

WO 2006/085599 A1#61204316 Most Cited · 1 citations0.1/yr · PR 0.75PendingWO · Application
Two-pack-type seizing inhibitor for hot plastic working and process for producing seamless tube with the same

A seizing inhibitor for hot plastic working which is a two-pack type inhibitor consisting of: a first aqueous solution containing sodium silicate in an amount of 10-30 mass% in terms of anhydride amount based on the whole first aqueous solution; and a second aqueous solution…

WO 2007/114173 A1#54526135 Most Cited · 1 citations0.1/yr · PR 0.81PendingWO · Application
Mandrel bar for rolling of high alloy, method for surface treatment of the mandrel bar, method for manufacture of the mandrel bar, and method for operation of seamless steel pipe production apparatus

Disclosed is a method for the surface treatment of a mandrel bar for use in the hot rolling of a high alloy steel seamless pipe, which comprises performing the scaling hot treatment of a mandrel bar and performing 50 passes or more of rolling of a common steel having a Cr…

WO 2007/138914 A1#48532736 Most Cited · 1 citations0.1/yr · PR 0.91PendingWO · Application
Process for producing seamless stainless-steel pipe

A process for producing a seamless pipe which comprises conducting a piercing rolling step, a drawing rolling step with a mandrel bar, and a sizing rolling step and subsequently conducting a product heat treatment. In the process, when the weight per unit area of the graphite…

WO 2008/081864 A1#61997867 Most Cited · 1 citations0.1/yr · PR 0.74PendingWO · Application
Method of application of lubricating oil to mandrel bar, method of control of thickness of lubricating oil on mandrel bar, and method of production of seamless steel pipe
Inventors: Saito Kenichi, Iida SumioAssignee: Sumitomo Metal Ind, Saito KenichiFiled 2007-12-27

In the application of a non-graphite lubricating oil comprising 10 to 70 mass% of an oxide-type layered compound and 30 to 90 mass% of boric acid onto a mandrel bar, the thickness of the lubricating oil is determined based on a master curve as determined at a predetermined…

US 2006130548 A1#79993027 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Cr-plated mandrel bar for manufacturing hot seamless tube and method of manufacturing the same

By employing a Cr-plated mandrel bar for producing hot seamless tubes according to the present invention wherein centerline average roughness Ra in axial and circumferential directions as well as maximum depth Rv in axial and circumferential directions is specified and further…

US 2013269407 A1#115206486 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method for producing seamless steel tube/pipe

When performing piercing-rolling by use of a plug with a protection film on its surface, applying a lubricant made of an aqueous solution containing a total of 5 to 30% mass % of one or more of boron oxide, boric acid, and amine borate to the protection film on the plug surface,…

US 8,065,901 B2#105411655 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Mandrel bar for high-alloy rolling, method for surface treating a mandrel bar, method for producing mandrel bar, and method for operating seamless pipe mill
Inventors: Iida Sumio, Hidaka Yasuyoshi, Yoshizawa Mitsuru, Nakaike KojiAssignee: Iida Sumio, Hidaka YasuyoshiFiled 2008-09-24 · Granted 2011-11-29

A method for surface treating a mandrel bar used for hot rolling of high-alloy seamless steel pipe is provided. The method includes heat treating the mandrel bar to develop a scale, and after heat treatment, rolling ordinary steel comprising 8% or less of chromium for at least…

US 8,082,767 B2#63304392 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Lubricant for hot metal working and powder lubricant composition for hot metal working
Inventors: Sasaki Kenichi, Iida Sumio, Mori ShizuoAssignee: Sasaki Kenichi, Iida SumioFiled 2007-03-23 · Granted 2011-12-27

The present invention provides a lubricant for hot metal working which is capable of inhibiting generation of white scale, attributed to the lubricant, on the surface of a workpiece material and is capable of improving lubricity to obtain favorable appearance of the finished…