Patents
US 8,293,168 B2#59131460 Most CitedActiveUnited States (USPTO)Utility

Nanocomposites with high thermoelectric figures of merit

1Forward Citations (#59131460 Global)
0.1/yrCitation Velocity (#51168576 Global)
0.78Citation PageRank (#59131460 Global)
50Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention is generally directed to nanocomposite thermoelectric materials that exhibit enhanced thermoelectric properties. The nanocomposite materials include two or more components, with at least one of the components forming nano-sized structures within the composite material. The components are chosen such that thermal conductivity of the composite is decreased without substantially diminishing the composite's electrical conductivity. Suitable component materials exhibit similar electronic band structures. For example, a band-edge gap between at least one of a conduction band or a valence band of one component material and a corresponding band of the other component material at interfaces between the components can be less than about 5k B T, wherein k B is the Boltzman constant and T is an average temperature of said nanocomposite composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of synthesizing a thermoelectric nanocomposite semiconductor composition, comprising generating a powder mixture comprising two or more sets of nano-sized semiconductor structures, applying a compressive pressure to said mixture while flowing current through said mixture to heat the mixture to a selected temperature for a time duration selected to cause compaction of said sets of nano-sized structures into the thermoelectric nanocomposite semiconductor composition having a matrix with nano-sized inclusions.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said compressive pressure is in a range of about 10 to about 1000 MPa.

  3. Claim 3Independent Claim

    A method of synthesizing a thermoelectric nanocomposite semiconductor composition, comprising generating a powder mixture comprising two or more sets of nano-sized semiconductor structures, applying a compressive pres

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,588,520 APowder pressed thermoelectric materials and method of making same198627
US 5,069,868 AMethod for producing thermoelectric elements199124
US 5,246,504 AThermoelectric material199337
US 5,318,743 AProcesses for producing a thermoelectric material and a thermoelectric element199448
US 5,531,936 AAlkali metal quaternary chalcogenides and process for the preparation thereof199632
JP H0925526 AProduction of oxide grain dispersed metal matrix composite—12
DE 19,627,389 A1Verfahren zur Herstellung von Verbundwerkstoffen auf Metallbasis mit Oxidteilchendispersion—8
US 5,614,128 AAlkali metal quaternary chalcogenides and process for the preparation thereof199728
US 5,618,471 AAlkali metal quaternary chalcogenides and process for the preparation thereof199730
US 5,723,799 AMethod for production of metal-based composites with oxide particle dispersion199835
JP H1070315 AManufacture of thermoelectric material—18
US 5,763,293 AProcess of fabricating a thermoelectric module formed of V-VI group compound semiconductor including the steps of rapid cooling and hot pressing199829
US 5,883,563 AThermo-electric material having mean crystal grain diameter nor greater than 50 microns and mean aspect ratio between 1 and 3 for large figure of merit and thermo-electric element using the same199937
US 5,897,945 AMetal oxide nanorods1999497
US 5,929,351 ACo-Sb based thermoelectric material and a method of producing the same199948
US 5,965,841 AThermoelectric conversion material and a process for producing the same199920
US 5,973,050 AComposite thermoelectric material199959
US 5,989,487 AApparatus for bonding a particle material to near theoretical density199935
US 6,013,204 AAlkali metal chalcogenides of bismuth alone or with antimony200040
WO 0,012,600 A1Composite thermoelectric material—7
US 6,060,656 ASi/SiGe superlattice structures for use in thermoelectric devices200074
US 6,069,312 AThermoelectric materials with filled skutterudite structure for thermoelectric devices200052
JP 2000261052 AManufacture for thin-film thermoelectric conversion element and the thin-film thermoelectric conversion element—9
US 6,147,293 AProcess for producing sintered thermoelectric semiconductor and sintered thermoelectric semiconductor200012
US 6,207,886 B1Skutterudite thermoelectric material thermoelectric couple and method of producing the same200164
US 6,222,242 B1Thermoelectric semiconductor material and method of manufacturing same200139
US 6,225,548 B1Thermoelectric semiconductor compound and method of making the same200141
US 6,235,981 B1P-type thermoelectric converting substance and method of manufacturing the same20019
US 6,274,802 B1Thermoelectric semiconductor material, manufacture process therefor, and method of hot forging thermoelectric module using the same200146

Non-Patent Literature (5)

  • Bennett, G.L., "Space Applications, in CRC Handbook of Thermoelectrics," Ed.D.M. Rowe, CRC Press, Boca Raton, pp. 515-537 (1995).
  • Bettotti et al., "Silicon nanostructures for photonics," J. Phys.: Condens. Matter 2002, 14, 8253-8281.
  • Borca-Tasciuc et al., "Thermal Conductivity of InAs/AlSb Superlattices," Microscale Thermophysical Engineering, 5, pp. 225-231 (2001).
  • Borca-Tasciuc et al., "Thermal conductivity of symmetrically strained Si/Ge superlattices," Superlattices and Microstructures, vol. 28, pp. 119-206 (2000).
  • Bostedt et al., "Evidence for cubic phase in deposited germanium nanocrystals," J. Phys.: Condens. Matter 2003, 15, 1017-1028.