Process of fabricating a thermoelectric module formed of V-VI group compound semiconductor including the steps of rapid cooling and hot pressing
Abstract
A process wherein powder of p/n-type semiconductor thermoelectric materials expressed as (Bi, Sb) 2 (Te, Se) 3 is hot pressed under the pressure equal to or greater than 400 kgf/cm 2 at 200 degrees to 400 degrees in centigrade for a time period between {(-T/5)+90} minutes and 150 minutes or at 400 degrees to 500 degrees in centigrade for a time period between 5 minutes and 150 minutes so as to increase the figure of merit by virtue of the strain left in the crystal and/or micro crystal grain, and pieces of p/n-type semiconductor thermoelectric material are assembled with electrodes so as to obtain a thermoelectric module for a high thermoelectric conversion efficiency.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 29.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process of fabricating a thermoelectric module, comprising: a) preparing molten semiconductor thermoelectric materials each containing at least one first element selected from the group consisting of bismuth and antimony and at least one second element selected from the group consisting of tellurium and selenium; b) rapidly cooling said molten semiconductor thermoelectric materials so as to solidify one of said semiconductor thermoelectric materials and another of said semiconductor thermoelectric materials into a first mixture of powder and laminae of a first conductivity type and a secon
Technical Overview & Description