Patents
US 8,230,702 B2#34143353 Most CitedActiveUnited States (USPTO)Utility

Glass-tube extended-baking process

3Forward Citations (#34143353 Global)
0.2/yrCitation Velocity (#32502555 Global)
0.93Citation PageRank (#45958592 Global)
32Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Disclosed is a method of heat treating quartz glass deposition tubes at between 900° C. and 1200° C. for at least 115 hours. The resulting deposition tubes are useful in forming optical preforms that can yield optical fibers having reduced added loss.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 32 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An extended-baking method for improving the optical properties of a glass deposition tube, comprising the step of subjecting the glass deposition tube to heat-treatment at 900° C. or higher under reduced pressure of 100 millitorr or less for at least 115 hours.

  2. Claim 2Depends on #1

    A method according to claim 1 , wherein the step of subjecting the glass deposition tube to heat-treatment comprises subjecting the glass deposition tube to heat-treatment of between about 1000° C. and 1200° C. for about 150 hours or more.

  3. Claim 3Depends on #1

    A method according to claim 1 , wherein the step of subjecting the glass deposition tube to heat-treatment comprises subjecting the glass deposition tube to heat-treatment under reduced pressure of between about 1 millitorr and 50 millitorr.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (32)

PatentTitleYearCitations
US 3,782,914 AHeat treating optical waveguides for oh ion removal197421
US 4,388,095 AMethod of producing a glass layer on an interior surface of a hollow body198316
US 4,504,297 AOptical fiber preform manufacturing method198533
US 5,106,402 AMethod of manufacturing a monomode optical fiber199269
JP H06293530 AProduction of optical fiber preform—2
CN 1,273,948 AProcess for preparing low-hydroxyl quartz tube—12
US 2002144521 A1Method of manufacturing large capacity preforms by MCVD—26
US 2003031441 A1Optical fibre and method of manufacturing an optical fibre—11
US 6,530,244 B1Optical fiber preform having OH barrier and fabrication method thereof200323
US 6,546,757 B1Liquid spray pyrolysis method for the fabrication of optical fiber preforms, with reactant mixing200330
US 6,687,444 B2Decreased H2 sensitivity in optical fiber20046
CN 1,472,151 AManufacture of single mode oplical fibers—21
US 6,739,155 B1Quartz making an elongated fused quartz article using a furnace with metal-lined walls200427
US 2004146258 A1Optical fiber, dispersion compensator, optical transmission line and optical communications system—13
US 6,799,440 B2Optical fiber deposition tube fused in deuterium atmosphere for attenuation improvement20049
US 2005000253 A1Method of manufacture of low water peak single mode optical fiber—38
US 2005081565 A1Method of producing higher-purity glass element, high-purity glass element, and production method and device for glass tube—10
US 2005120751 A1Method for manufacturing a preform for optical fibres, as well as a method for manufacturing optical fibres—20
US 2005172676 A1Method for the production of a cylindrical quartz glass body having a low oh content—16
US 6,952,516 B2Low attenuation optical fiber20058
US 2005223747 A1Method for making low loss optical fiber—6
US 6,988,379 B2Method of manufacturing large capacity preforms by MCVD200612
WO 2006/082983 A2Process for producing synthetic quartz glass and synthetic quartz glass for optical member—7
US 7,092,610 B2Optical fiber for attenuating optical signal20066
US 2006191294 A1Synthetic silica glass tube for the production of a preform, method for producing the same in a vertical drawing process and use of said tube—23
US 2007125129 A1Optical fiber having low and uniform optical loss along the entire length and method for fabricating the same—13
EP 1,942,081 A2Extended baking process for quartz glass deposition tubes.—2

Non-Patent Literature (5)

  • Chinese Office Action in counterpart Chinese Application No. 2011060100627640 dated Jun. 7, 2011, pp. 1-7.
  • Decision to Grant Patent in counterpart European Application No. 08000008 dated Oct. 13, 2011, pp. 1-2.
  • Extended European Search Report in counterpart European Application No. 08000008 dated Mar. 4, 2010, pp. 1-7.
  • Intention to Grant Patent in counterpart European Application No. 08000008 dated Apr. 26, 2011, pp. 1-4.
  • Intention to Grant Patent in counterpart European Application No. 08000008 dated Mar. 4, 2010, pp. 1-4.