Optical fiber for attenuating optical signal
Abstract
In order to supply the optical fiber for attenuating optical signal enable the attenuation amount to become flat in wide wavelength scope, simultaneously adding at least two kinds of dopants for attenuating optical signal over the core and the cladding of the optical fiber. Then, properly adjusting the kind and the concentration of dopants for manufacturing the optical fiber 1 for attenuating optical signal; simultaneously adding the dopant enabling the absorption of optical signal to increase with the wavelength become long and the dopant enabling the absorption of optical signal to decrease with the wavelength become long. As the dopant, it is desired to select at least two kinds of transitional metals from Co, Ni, Cr, V, Fe, Mn, Tb and Tm. Further, as the doped area, it is desired to dope the 6 times of the center portion of the core from the center of the core.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An optical fiber for attenuating an optical signal comprising a core and a cladding, wherein n (n≧2) kinds of dopants are included in the optical fiber for attenuating the optical signal, wherein the concentration Wj (j=1, 2, 3, . . . , n) in weight % is adjusted, with respect to a wavelength λi (i=1, 2, . . . , m; m≧2), to satisfy the following expressions 1 and 2; 0.9 < α ( λ i
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗