Method of producing reduced iron cast, and method of producing pig iron
Abstract
In a method of producing a reduced iron cast, a cast of a powder which includes total iron of 40% or more and an atomic molar amount of fixed carbon of 0.7 to 1.5 times the atomic molar amount of oxygen compounded with metal oxide reduced in a carbon monoxide atmosphere at 1200° C. is reduced in a rotary hearth furnace. The method includes: producing, in an atmosphere at a maximum temperature of 1200° C. to 1420° C. at a ratio of carbon monoxide to carbon dioxide of 0.3 to 1.2 in the reduced zone, a reduced iron-containing material in which a ratio of metal iron is 50 mass % or more and a ratio of carbon is 5 mass % or less; and compression-molding the reduced iron-containing material at a temperature of 500° C. to 800° C. by a roller-type mold.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing pig iron, comprising: reducing a cast of a powder which includes total iron of 40% or more and an atomic molar amount of fixed carbon of 0.7 to 1.5 times the atomic molar amount of oxygen compounded with metal oxide reduced in a carbon monoxide atmosphere at 1200° C. in a rotary hearth furnace to produce a reduced iron-containing material having a metal iron ratio of 50 mass % or more and a carbon ratio of 5 mass % or less in an atmosphere at a maximum temperature of 1200° C. to 1420° C. at a ratio of carbon monoxide to carbon dioxide of 0.3 to 1.2 in the reduced zone, an
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| EP 4,632,088 A1 | Hot briquetted iron | — | 0 |
References Cited — Backward Prior Art (24)
Non-Patent Literature (5)
- Canadian Office Action dated Aug. 8, 2011, for Canadian Application No. 2,698,234.
- Chinese Office Action dated Apr. 29, 2011, in Chinese Application No. 200880105460.3.
- Extended European Search Report dated Nov. 4, 2010 for corresponding European Application No. 08829382.4.
- International Search Repot PCT/ISA/210, mailed Dec. 16, 2008.
- Kurunov I.F. et al, "State and aspects of iron metallurgy without blast furnace", Chermetinformatsiya, 2002, pp. 80-81.