Abstract

There is provided a method of producing reduced iron compacts with high crushing strength, low powderization and a high reduction rate in a solid reduction-type firing reducing furnace such as a rotary hearth-type reducing furnace, as well as reduced iron compacts obtained by the method and a method of melt-reducing the reduced iron compacts in a blast furnace. In the method of producing reduced iron compacts, the atomic molar ratio of carbon to oxygen chemically combined with iron, manganese, nickel, zinc and lead, in raw material powder comprising a mixture of iron oxide-containing powder and carbon-containing powder, or the ferric oxide content of the raw material powder, is in a specified range, the compact is produced so as to give a porosity in a given range, and the compact is put on the hearth of a reducing furnace equipped with a rotating hearth and is heated for heating reduction by the heat from the combustion gas in the upper part of the furnace, for firing reduction at above a prescribed temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a reduced iron compact in a rotary hearth reducing furnace, characterized by producing a compact with a porosity of 20-33% using a raw material powder wherein the total iron content is at least 40 mass % and wherein, among the included elements, the atomic molar ratio of carbon to oxygen chemically combined with iron and one or more members selected from the group consisting of manganese, nickel, zinc and lead is in the range of 0.5-1.5, putting said compact on the hearth of a reducing furnace equipped with a rotating hearth, and heating it for heating reduction by the he

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Notice of Reasons for Rejection English Translation Sep. 14, 2004 Japanese Patent App No. 2001-269794.
  • Notice of Reasons for Rejection English Translation Sep. 14, 2004 Japanese Patent App No. 2001-279056.