High crashworthiness Al-Si-Mg alloy and methods for producing automotive casting
Abstract
The present invention provides a casting having increased crashworthiness including an aluminum alloy of about 6.0 wt % to about 8.0 wt % Si; about 0.12 wt % to about 0.25 wt % Mg; less than or equal to about 0.35 wt % Cu; less than or equal to about 4.0 wt % Zn; less than or equal to about 0.6 wt % Mn; and less than or equal to about 0.15 wt % Fe, wherein the cast body is treated to a T5 or T6 temper and has a tensile strength ranging from 100 MPa to 180 MPa and has a critical fracture strain greater than 10%. The present invention further provides a method of forming a casting having increased crashworthiness.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
An Al—Si—Mg alloy composition used to produce a cast product having a critical fracture strain of at least about 10%, the alloy comprising: about 6.0 wt % to about 7.8 wt % Si; about 0.10 wt % to about 0.18 wt % Mg; less than or equal to about 0.35 wt % Cu; less than or equal to about 0.6 wt % Mn; less than or equal to about 0.15 wt % Fe; and a balance of aluminum and impurities; wherein, the composition is capable of producing a cast product having a critical fracture strain of at least about 10% and a tensile yield strength of at least 100 MPa when the composition undergoes a heat treating p
- Claim 2Depends on #1
The alloy of claim 1 , further comprising at least one silicon modifier in an amount less than or equal to 0.02 wt %, wherein the modifier comprises Ca,