Reducing the susceptibility of alloys, particularly aluminium alloys, to stress corrosion cracking
Abstract
A method is described of thermally treating the 7,000 series aluminum alloys that have been subjected to a solution heat treatment at a high temperature and then to an ageing treatment at a lower temperature, thereby hardening the alloy but likewise producing therein a susceptibility to stress-corrosion cracking. The novel method comprises the steps of (1) subjecting the alloy to a retrogression heat treatment for a short period of time at a temperature above the age-hardening temperature of the alloy but below the solution heat treatment temperature, and (2) subsequently subjecting the alloy to a re-ageing heat treatment for a substantially longer period of time at the age-hardening temperature of the alloy. This method substantially reduces the susceptibility of the alloy to stress-corrosion cracking while retaining its original strength.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 62.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A METHOD OF SUBSTANTIALLY REDUCING THE SUSCEPTIBILITY TO STRESS-CORROSION CRACKING OF THE 7,000 SERIES ALUMINUM ALLOYS CONTAINING ZINC, MAGNESIUM, AND COPPER, WHILE STILL RETAINING THEIR ORIGINAL MECHANICAL STRENGTH, WHILE ALLOYS HAVE BEEN SUBJECTED TO A SOLUTION HEAT TREATMENT AT A HIGH TEMPERATURE AND THEN TO AN AGING TREATMENT AT A LOWER TEMPERATURE THEREBY HARDENING THE ALLOY BUT LIKEWISE PRODUCING THEREIN A SUSCEPTIBILITY TO STRESS-CORROSION CRACKING, COMPRISING THE STEPS OF: A. SUBJECTING THE ALLOY TO A RETROGRESSION HEAT TREATMENT FOR A FEW SECONDS TO A FEW MINUTES AT A TEMPERATURE OF F
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗