Patents
US 8,076,387 B2#26702361 Most CitedActiveUnited States (USPTO)Utility

High modulus crosslinked polyethylene with reduced residual free radical concentration prepared below the melt

4Forward Citations (#26702361 Global)
0.3/yrCitation Velocity (#27676799 Global)
1.17Citation PageRank (#33407710 Global)
46Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention provides an irradiated crosslinked polyethylene containing reduced free radicals, preferably containing substantially no residual free radical. Disclosed is a process of making irradiated crosslinked polyethylene by irradiating the polyethylene in contact with a sensitizing environment at an elevated temperature that is below the melting point, in order to reduce the concentration of residual free radicals to an undetectable level. A process of making irradiated crosslinked polyethylene composition having reduced free radical content, preferably containing substantially no residual free radicals, by mechanically deforming the polyethylene at a temperature that is below the melting point of the polyethylene, optionally in a sensitizing environment, is also disclosed herein.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A crosslinked polyethylene composition made by a process comprising the steps of: a) irradiating polyethylene at a temperature that is below the melting point of the polyethylene, wherein the polyethylene is irradiated at a dose level between about 1 and about 10,000 kGy; b) heating the irradiated polyethylene at a temperature that is above room temperature and below the melting point of the irradiated polyethylene, thereby reducing the residual free radical concentration; c) mechanically deforming the polyethylene from step b) at a temperature that is above room temperature and below the melt

  2. Claim 2Depends on #1

    The crosslinked polyethylene composition of claim 1 , wherein the polyethylene is ultra-hig

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (46)

PatentTitleYearCitations
US 4,113,595 AProcess for producing molded product composed of crosslinked resin or crosslinked-resin coated material on a substrate by means of electron beam197828
US 4,587,163 APreparation of ultra high molecular weight polyethylene morphologies of totally fused particles with superior mechanical performance1986122
JP 4,587,163 B2検索システム、検索方法、報告システム、報告方法、及びプログラム20100
US 5,030,402 AProcess for producing a new class of ultra-high-molecular-weight polyethylene orthopaedic prostheses with enhanced mechanical properties1991127
US 5,414,049 ANon-oxidizing polymeric medical implant1995256
US 5,428,079 ASolution of ultra-high molecular weight polyethylene199569
US 5,449,745 ANon-oxidizing polymeric medical implant1995113
WO 9,609,330 A1Ultrahigh-molecular-weight polyethylene molding for artificial joint and process for producing the molding—20
US 5,508,319 AHigh melt strength, ethylene polymer, process for making it, and use thereof199686
US 5,543,471 ANon-oxidizing polymeric medical implant199676
US 5,577,368 AMethod for improving wear resistance of polymeric bioimplantable components1996146
US 5,594,041 AMethods for increasing structural integrity of polymers and polymers treated by such methods199716
US 5,650,485 ANon-oxidizing polymeric medical implant199797
WO 9,729,793 A1Radiation and melt treated ultra high molecular weight polyethylene prosthetic devices—124
WO 9,801,085 A1Crosslinking of polyethylene for low wear using radiation and thermal treatments—66
US 5,728,748 ANon oxidizing polymeric medical implant1998107
US 5,753,182 AMethod for reducing the number of free radicals present in ultrahigh molecular weight polyethylene orthopedic components1998124
US 5,824,411 ASelf-reinforced ultra-high molecular weight polyethylene composites199878
US 5,834,113 ASelf-reinforced ultra-high molecular weight polyethylene composite medical implants199847
US 5,879,400 AMelt-irradiated ultra high molecular weight polyethylene prosthetic devices1999280
US 6,017,975 AProcess for medical implant of cross-linked ultrahigh molecular weight polyethylene having improved balance of wear properties and oxidation resistance2000206
US 6,143,232 AMethod of manufacturing an articulating bearing surface for an orthopaedic implant200050
US 6,165,220 AWear resistant surface-gradient crosslinked polyethylene2000125
US 6,168,626 B1Ultra high molecular weight polyethylene molded article for artificial joints and method of preparing the same200189
US 6,174,934 B1Non-oxidizing polymeric medical implant200175
WO 0,105,337 A1Polyethylene hip joint prosthesis with extended range of motion—67

Non-Patent Literature (2)

  • Jasty, Document dated Jan. 11, 1999.
  • Jasty, Document dated Jan. 30, 1999.