hottub.patents
US 5,449,745 A#44539 Most CitedExpiredUnited States (USPTO)Utility

Non-oxidizing polymeric medical implant

1Forward Citations (#44539 Global)
0.0/yrCitation Velocity (#65745 Global)
1.96Citation PageRank (#44401 Global)
19Prior Art Cited
3Structured Claims
0Drawings / Sheets

Abstract

A medical implant made of polymeric material having an increased oxidation resistance is formed by a method including the steps of placing a resin powder in a sealed container. A substantial portion of the oxygen is removed from the sealed container by either a vacuum, an oxygen absorbent or by flushing with inert gas. The container is then repressurized with a gas such as nitrogen, argon, helium or neon so that long term storage may be possible. On use, the resin is transferred to a forming device which both melts and forms the resin in an oxygen reduced atmosphere to produce a polymeric raw material such as a rod or bar stock. The medical implant is then formed from this raw material annealed and sealed in an air-tight package in an oxygen reduced atmosphere. The implant is then radiation sterilized and thereafter annealed in the package for a predetermined time and temperature sufficient to form cross-links between any free radicals in neighboring polymeric chains.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 1.

Claims (3)

  1. Claim 1Independent Claim

    A method for producing raw polymeric matedal having improved oxidation resistance from a plastic resin powder for a medical implant comprising the steps of: placing the resin in a sealed container; removing a substantial portion of the oxygen from said sealed container; repressurizing the sealed container with a gas selected from the group consisting of nitrogen, argon, helium and neon and a combination thereof; then transferring said resin to a forming device which both melts and forms said resin in an oxygen reduced atmosphere to produce the raw material; and thereafter annealing the

  2. Claim 2Depends on #1

    The method as set forth in claim 1 wherein the oxygen content of the atmosphere in said sealed container is reduced to less than 1%.

  3. Claim 3Independent Claim

    The method as set for

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (19)

Non-Patent Literature (5)

  • "Combined Chem. & Mechanical Effects on Free Radicals in UHMWPE . . . " M. Janan et al., Jnl. Biomed. Mat. Res., vol. 25, 1991, pp. 1005-1017.
  • "Polypropylene Degradation by γ-Irradiaton in Air" D. Carlsson et al, Amer. Chemical Society, 1985.
  • "Radiation Effects on Polymers", R. Clough & S. Shalaby ACS Symposium, Washington, D.C., Aug. 26,-31, 1990.
  • "Radical Migration as an Elementary Process in Degradation" J. Sohma, Pure and Appl. Chem., vol. 55, No. 10, pp. 1595-1601, 1983.
  • Combined Chem. & Mechanical Effects on Free Radicals in UHMWPE . . . M. Janan et al., Jnl. Biomed. Mat. Res., vol. 25, 1991, pp. 1005 1017.