High manganese duplex stainless steel having superior hot workabilities and method manufacturing thereof
Abstract
A high manganese duplex stainless steel with excellent hot workability, comprising (in weight %): less than 0.1% of C; 0.05-2.2% of Si; 2.1-7.8% of Mn; 20-29% of Cr; 3.0-9.5% of Ni; 0.08-0.5% of N; less than 5.0% of Mo and 1.2-8% of W, alone or composite; the balance Fe and inevitable impurities; and a method for manufacturing the duplex stainless steel, comprising the steps of: solution heating the duplex stainless steel composition at a temperature of 1,050 to 1,250° C., hot working at a starting temperature of 1,130 to 1,280° C. and then ending at a temperature greater than 1,000° C., and then cooling within the temperature range from 1,000 to 700° C. at a cooling rate of more than 3° C./min. The duplex stainless steel exhibits a reduction in area of more than 50% at 1,050° C., and possesses a yield strength of more than 400 MPa, and a corrosion rate of less than 0.36 mm/year, after solution heating.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A high manganese duplex stainless steel with excellent hot workability, comprising (in weight %): 0.018%-0.1% of C; 0.05-2.2% of Si; 3.52-7.8% of Mn; 20-27.8% of Cr; 3.0-9.5% of Ni; 0.08-0.5% N; up to 4.15% Mo; 3.41-8% W; less than 1.0% Cu; less than 0.4% Ti; the balance Fe and inevitable impurities and wherein Mo and W meet the condition: Mo+0.5W=1.0-4.4% and having a reduction in area of 50% or more when measured at 1,050° C. and a corrosion rate of less than 0.36 mm/year as determined by weight loss after exposure in a 10% FeCl 2 .6H 2 O solution for 72 hours at room temperature.
- Claim 2Depends on #1
The high manganese duplex stainless steel as set forth in claim 1 , wherein the content of Mo is 1.0-4.15%.
- Claim 3Depends on #1
The high manganese duplex stainless steel as set forth in claim 1 , wherein the contents of Mo and Mn meet the following formula: 44.37+9.806 [% Mn]−3.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (28)
Non-Patent Literature (5)
- "Duplex Stainless Steels, Microstructure, Properties and Applications", 1997, 3 pp.; Robert N. Gunn, Ed.; Abington Publishing; Cambridge, England.
- Bogdanova, T.M. et al., "The Workability of Austenitic Manganese Steels During the Production of Hot Rolled Pipes", Structure and Properties of Nonmagnetic Steels (Struktura i Svoystua Nemagnitnykh Steley, 1982, pp. 185-190, Nauka, Moscow, USSR.
- Davis et al., The ASM Handbook, Aug. 1991, vol. 4, pp. 91-92.
- G.J. Adetunji, R.G. Faulkner and E.A. Little, "Quenching-rate determination for standard steel tensile specimens", J Mater Sci 26 (1991), pp. 1847-1850.
- Kömi, J.I. et al., "Effects of Sulphur, Phosphorus and Cerium on the Hot Workability of a Ferritic-Austenitic Stainless Steel", Proceedings of International Conference on Stainless Steels, 1991, Chiba, ISIJ, pp. 807-814.