Ferrite-austenite stainless steel castings having an improved erosion-corrosion resistance

13Forward Citations (#7189648 Global)
0.3/yrCitation Velocity (#27251440 Global)
6.88Citation PageRank (#1968595 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Ferrite-austenite stainless steel castings having an improved erosion-corrosion resistance consist by weight percentage of not more than 0.1% of C, 0.2-3% of Si, not more than 2% of Mn, 2.2-4% of Cu, 3-9% of Ni, 20-30% of Cr, 2-6% of Mo, 0.08-0.25% of N, 0.12-0.3% of Sn, at least one of 0-2% of Nb, 0-1% of Ti, 0-2% of Ta, 0-1% of Zr and 0-1.5% of V and remainder of Fe, and are obtained by solution heat treatment at 1,000°-1,150° C in such a manner that Cr- and Ni-equivalents lie within an area represented by the area ABCD shown in FIG. 1 of the accompanying drawings.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A ferrite-austenite stainless steel casting having an improved erosion-corrosion resistance, consisting by weight percentage of not more than 0.1% of carbon, 0.2-3% of silicon, not more than 2% of manganese, 2.2-4% of copper, 3-9% of nickel, 20-30% of chromium, 2-6% of molybdenum, 0.08-0.25% of nitrogen, 0.12-0.3% of tin, 0-2% of niobium, 0-1% of titanium, 0-2% of tantalum, 0-1% of zirconium, 0-5% of vanadium and remainder of iron; said stainless steel casting being obtained by solution heat treatment at a temperature of 1,000-1,150° C in such a manner that chromium-and nickel-equivalents lie

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Metals Abstracts, Sep. 1971, p. 1327, Abstract #35-1078.