Polyolefin composition having a high balance of stiffness, impact strength and elongation at break and low thermal shrinkage
Abstract
Polymer composition showing an improved balance of flexural modulus, IZOD impact strength and elongation at break comprising (percent by weight): A) a polymer blend comprising: A1) 50-70% of a crystalline propylene homopolymer or copolymer; and A2) 30-50% of one or more copolymer(s) of ethylene with one or more C 4 -C 10 α-olefin(s) containing from 15 to 35% of said C 4 -C 10 α-olefin(s); said polymer blend (A) having values of MFR equal to or higher than 10 g/10 min., a total content C 4 -C 10 α-olefin(s) equal to or higher than 8% and an intrinsic viscosity value of the fraction soluble in xylene at room temperature of from 1.3 to 2 dl/g, the amounts of (A1) and (A2) being referred to the total weight of the polymer blend; and optionally B) 1-15% of an elastomeric polymer different from A2), having a hardness (Shore A, ASTM D-2240) value equal to or lower than 90 points; and/or C) 0.5-20% of a mineral filler; the amounts of optional components (B) and (C) being referred to the total weight of the composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A polymer composition comprising (percent by weight): (A) a polymer blend comprising: (A1) 50-70% of a crystalline propylene homopolymer or copolymer comprising up to 5% of ethylene and/or at least one C 4 -C 10 α-olefin, said homopolymer or copolymer comprising a MFR value (230° C., 2.16 kg) of from 50 to 200 g/10 min. and a content of fraction soluble in xylene at room temperature of 7% or less; and (A2) 30-50% of at least one copolymer of ethylene with at least one C 4 -C 10 α-olefin, the copolymer of ethylene comprising from 15 to 35% of said C 4 -C 10 α-olefin; said polymer blend (A) c
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- J. Randall, "3,4 Monomer Distributions and Number-Average Sequence Lengths in Ehtylene Propylene Copolymers," Polymer Sequence Determination; Carbon-13 NMR Method, p. 53-58 (1977).
- J. Randall, "A Review of High Resolution Liquid13Carbon Nuclear Magnetic Resonance Characterizations of EthyleneBased Polymers," JMS-Rev. Macromol. Chem. Phys, C29(2&3), p. 201-317 (1989).
- J. Wolters, "Polyolefin-Elastomere; Moderne Katalysatoretchnik steht Pate fur Thermoplaste mit Kautscuk-Eigenschaften," Kuntstoffe, vol. 84, p. 446-450 (1994).
- M. Kakugo et al., "13C NMR Determination of Monomer Sequence Distribution in Ethylene Propylene Copolymers Prepared withdelta-TiCI3-AI(C2H5)2CI," Macromolecules, vol. 15(4), p. 1150-1152 (1982).
- M. Kakugo et al., "13C NMR Determination of Monomer Sequence Distribution in Ethylene Propylene Copolymers Prepared withδ-TiCI3-AI(C2H5)2CI," Macromolecules, vol. 15(4), p. 1150-1152 (1982).