A method of forming a conformal dielectric film having Si—N bonds on a semiconductor substrate by plasma enhanced chemical vapor deposition (PECVD) includes: introducing a nitrogen- and hydrogen-containing reactive gas and a rare gas into a reaction space inside which a semiconductor substrate is placed; applying RF power to the reaction space; and introducing a hydrogen-containing silicon precursor as a first precursor and a hydrocarbon gas as a second precursor in pulses into the reaction space wherein a plasma is excited, thereby forming a conformal dielectric film doped with carbon and having Si—N bonds on the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of forming a conformal dielectric film having Si—N bonds on a semiconductor substrate by plasma enhanced chemical vapor deposition (PECVD), which comprises: introducing a nitrogen- and/or hydrogen-containing reactive gas and a rare gas into a reaction space inside which the semiconductor substrate is placed; applying RF power to the reaction space; and introducing a hydrogen-containing silicon gas as a first precursor and a hydrocarbon gas as a second precursor separately, each precursor being introduced in pulses of less than 5-second duration into the reaction space while introducin

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the first precursor has a formula of Si α H β X γ , wherein α, β

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
US 5,801,104 AUniform dielectric film deposition on textured surfaces199828
US 6,017,779 AFabrication method for a thin film semiconductor device, the thin film semiconductor device itself, liquid crystal display, and electronic device2000100
US 2005181535 A1Method of fabricating passivation layer for organic devices—49
US 6,974,781 B2Reactor precoating for reduced stress and uniform CVD200526
US 2006019502 A1Method of controlling the film properties of a CVD-deposited silicon nitride film—15
US 7,092,287 B2Method of fabricating silicon nitride nanodots200617
US 2006199357 A1High stress nitride film and method for formation thereof—72
US 2007166999 A1Systems and methods of forming refractory metal nitride layers using disilazanes—10
US 2007251444 A1PEALD Deposition of a Silicon-Based Material—50
US 7,294,582 B2Low temperature silicon compound deposition200741
US 7,297,641 B2Method to form ultra high quality silicon-containing compound layers200718
US 2008003838 A1Deposition of complex nitride films—31
US 2008242116 A1Method for forming strained silicon nitride films and a device containing such films—87
US 2008317972 A1Method for depositing thin films by mixed pulsed cvd and ald—60
US 2009311857 A1Method to form ultra high quality silicon-containing compound layers—36
US 2010124621 A1Method of Forming Insulation Film by Modified PEALD—61
US 2010144162 A1METHOD OF FORMING CONFORMAL DIELECTRIC FILM HAVING Si-N BONDS BY PECVD—6
US 2010184302 A1Method of Forming Conformal Dielectric Film Having Si-N Bonds by PECVD—20

Non-Patent Literature (4)

  • Final Office Action for U.S. Appl. No. 12/357,174 dated Sep. 1, 2010.
  • Non-Final Office Action for U.S. Appl. No. 12/357,174, dated Apr. 1, 2010.
  • Non-Final Office Action for U.S. Appl. No. 12/553,759 dated Dec. 15, 2010.
  • Notice of Allowance for U.S. Appl. No. 12/357,174 dated Dec. 13, 2010.