Fabrication method for a thin film semiconductor device, the thin film semiconductor device itself, liquid crystal display, and electronic device

100Forward Citations (#238892 Global)
3.9/yrCitation Velocity (#514698 Global)
9.17Citation PageRank (#1224402 Global)
31Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In order to fabricate a high performance thin film semiconductor device using a low temperature process in which it is possible to use low price glass substrates, a thin film semiconductor device has been fabricated by forming a silicon film at less than 450° C., and, after crystallization, keeping the maximum processing temperature at or below 350° C. In applying the present invention to the fabrication of an active matrix liquid crystal display, it is possible to both easily and reliably fabricate a large, high-quality liquid crystal display. Additionally, in applying the present invention to the fabrication of other electronic circuits as well, it is possible to both easily and reliably fabricate high-quality electronic circuits.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 100.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A fabrication process for fabricating a thin film semiconductor device, comprising: forming an underlevel protection layer comprising an insulating material formed on at least a portion of a substrate; forming a semiconductor film on the underlevel protection layer the semiconductor film being an active layer of a transistor; and melt crystallizing the semiconductor film, wherein a surface roughness of the underlevel protection layer has a center line mean roughness value of about 1.5 nm or less.

  2. Claim 2Independent Claim

    A fabrication process for fabricating a thin film semiconductor device using a single plasma enhanced chemical vapor deposition reactor, comprising: removing films adhered in a deposition chamber of said plasma enhanced chemical vapor deposition reactor; forming a passivation layer in said deposition chamber; placing at least one substra

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 100 total)

PatentTitleYearCitations
US 7,972,980 B2Method of forming conformal dielectric film having Si-N bonds by PECVD20116
US 2011223699 A1Wiring Material, Semiconductor Device Provided with a Wiring Using the Wiring Material and Method of Manufacturing Thereof—0
US 7,919,416 B2Method of forming conformal dielectric film having Si-N bonds by PECVD20113
US 2004253771 A1Semiconductor device having semiconductor circuit formed by semiconductor elements and method for manufacturing the same—20
US 2005035348 A1Bottom gate-type thin-film transistor and method for manufacturing the same—0
US 6,739,196 B2Cleanliness evaluation in sputter targets using phase20047
US 8,148,743 B2Semiconductor device including semiconductor circuit made from semiconductor element and manufacturing method thereof20120
US 6,689,646 B1Plasma method for fabricating oxide thin films200419
US 2004118675 A1Method for deteriming a critical size of an inclusion in aluminum or aluminum alloy sputtering target—0
US 2005012040 A1Method of fabrication of an infrared radiation detector and infrared detector device—22
US 2006038262 A1Semiconductor processing methods—0
US 6,863,733 B1Apparatus for fabricating thin-film semiconductor device200522
US 7,572,705 B1Semiconductor device and method of manufacturing a semiconductor device20096
US 7,507,996 B2Contact structure of a wiring and a thin film transistor array panel including the same20097
US 7,629,624 B2Active matrix EL device with sealing structure housing the device and the peripheral driving circuits20090

Non-Patent Literature (5)

  • Dec. 5, 1993, Institute of Electrical and Electronics Engineers, pp. 847 850, XP000481744.
  • Dec. 5, 1993, Institute of Electrical and Electronics Engineers, pp. 847-850, XP000481744.
  • Masatada Horiuchi et al, "One-Decade Reduction of PN-Junction Leakage Current Using Poly-SI Interlayered SOI Structures" Proceedings of the International Electron Devices Meeting, Wash, DC Dec. 5-8, 1993.
  • Masatada Horiuchi et al, One Decade Reduction of PN Junction Leakage Current Using Poly SI Interlayered SOI Structures Proceedings of the International Electron Devices Meeting, Wash, DC Dec. 5 8, 1993.
  • Masumo K et al., "Low-Temperature Preparation of Poly-SI TFT by AR Laser Annealing at High Scanning Speed" Electronics & Communications in Japan, Part II--Electronics, vol. 76, No. 9, Sep. 1, 1993, pp. 112-116, XP000447931.