Method and composition for controlling the viscosity of latex compositions that include fly ash
Abstract
The present invention is a method and composition for controlling the viscosity of latex compositions that include fly ash. The composition is an aqueous dispersion comprising water, at least one polymer latex, from about 50 to about 600 parts by weight fly ash per 100 parts by weight dry polymer, and a viscosity stabilizing composition that preferably comprises at least one borate compound. The method includes adding a viscosity stabilizing composition to an aqueous polymer latex composition that includes fly ash. The viscosity stabilizing composition can be used to produce a stirred viscosity of the aqueous dispersion 7 days after mixing that is less than 30% greater than the viscosity of the aqueous composition immediately after mixing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 1.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An aqueous dispersion comprising: (a) water; (b) at least one polymer dispersed in water; (c) from about 50 to about 600 parts by weight fly ash per 100 parts by weight dry polymer; and (d) a viscosity stabilizing composition comprising at least one borate compound, wherein the weight ratio of the at least one borate compound to the fly ash is from about 0.001 to about 0.02.
- Claim 2Depends on #1
The dispersion as claimed in claim 1 , comprising 0.1 to 10 parts by weight of the at least one borate compound per 100 parts by weight dry polymer.
- Claim 3Depends on #1
The dispersion as claimed in claim 1 , comprising about 0.5 to about 3 parts by weight of at least one borate compound per 100 parts by weight dry polymer.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗