Patents
US 6,964,997 B2#5472694 Most CitedExpiredUnited States (USPTO)Utility

Molded article for interior parts of a car

17Forward Citations (#5472694 Global)
0.8/yrCitation Velocity (#9085420 Global)
1.98Citation PageRank (#14809846 Global)
8Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to interior parts of a car comprising a new propylene resin composition. The present resin composition has good molding abilities and a good balance of physical properties as well as a good appearance, lower gloss and scratch resistance. Specifically, the present invention relates to a molded article for interior parts of a car comprising a polypropylene resin composition comprising the following components; a crystalline homopolypropylene having MFR of 500 to 3,000 g/10 min.; a polypropylene consisting of a crystalline homopolypropylene and an ethylene-propylene copolymer rubber having 45 to 80% by mass of a ethylene content; a polypropylene consisting of a crystalline homopolypropylene and an ethylene-propylene copolymer rubber having 25% by mass or more to below 45% by mass of a ethylene content; and an ethylene-α-olefin copolymer rubber.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 17.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A molded article for interior parts of a car comprising a polypropylene resin composition comprising the following components (A) to (D) wherein a total amount of the components (A) to (D) is 100% by mass or less: Polypropylene (A):

  2. Claim 5Independent Claim

    0 to 30% by mass of a crystalline homopolypropylene having an MFR of 500 to 3,000 g/10 min. determined by a melt flow rate measurement at 230° C. under 21.6 N load and a fraction soluble in boiling p-xylene of 6.0% by mass or less; Polypropylene (B): 10 to 50% by mass of a polypropylene comprising a crystalline homopolypropylene (B 1 ) and an ethylene-propylene copolymer rubber (B 2 ), said ethylene-propylene copolymer rubber (B 2 ) having an intrinsic viscosity of 4.0 to 7.0 dl/g at 135° C. in decalin and a content of ethylene of 45% by mass to 80% by mass, and said polypropylene (B) comprisi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Characterization of Microstructure and Fracture Behavior of Polypropylene/Elastomer Blends Containing Small Crystal in Elastomeric Phase, Rakao Nomura, et al., Journal of Applied Polymer Science, vol. 55, 1307-1315 (1995).