Glass composition for improved refining and method
Abstract
A soda-lime-silica based glass composition for manufacturing on a float line that has a faster refining rate due to the introduction of alkali earth oxides such as BaO, ZnO and/or SrO in the amount of from about 1-4% in total. These oxides replace part or all of the MgO in the base glass composition thereby decreasing the overall MgO content in the glass composition to about 2% or less. The glass can realize a lower viscosity at high temperatures so that refining of the melt may occur faster.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 31 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A glass comprising: a base glass portion of the glass comprising: Ingredient wt. % SiO 2 67-75% Na 2 O 10-20% CaO 5-15% Al 2 O 3 0-7% K 2 O 0-7%
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2010040812 A1 | Glass composition | — | 9 |
References Cited — Backward Prior Art (31)
Non-Patent Literature (5)
- Derwent Abstract 1983-794097, English Abstract SU 983090 A. Dec. 23, 1982.
- Derwent Abstract 1985-011223, English Abstract SU 1097572 A. Jun. 15, 1984.
- Derwent Abstract 1985-245831, English Abstract JP 60161350 A. Aug. 23, 1985.
- Derwent Abstract 1985-245832, English Abstract JP 60161352 A. Aug. 23, 1985.
- Derwent Abstract 1990-310119, English Abstract JP 02221137 A. Sep. 4, 1990.