Patents
US 6,878,652 B2#12192452 Most CitedExpiredUnited States (USPTO)Utility

Methods of adjusting glass melting and forming temperatures without substantially changing bending and annealing temperatures and glass articles produced thereby

9Forward Citations (#12192452 Global)
0.4/yrCitation Velocity (#18748980 Global)
1.57Citation PageRank (#21332844 Global)
27Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method is provided for adjusting, e.g., lowering, the melting and/or forming temperatures of a glass composition without substantially changing the bending and annealing temperatures of the glass composition. The method includes increasing the amount of CaO and decreasing the amount of MgO in the glass composition by the same or about the same amount.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 9.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A glass composition, comprising: a. SiO 2 70 to 75 weight percent b. Na 2 O 12 to 15 weight percent c. K 2 O 0 to 5 weight percent d. CaO>9 weight percent e. MgO<4 weight percent f. Al 2 O 3 0 to less than 1.6 weight percent g. SO 3 0 to 1 weight percent h. Fe 2 O 3 0 to less than 0.65 weight percent wherein SiO 2 +Al 2 O 3 ≧70 weight percent Na 2 O+K 2 O 12 to 15 weight percent CaO+MgO 12 to less than 13.4 weight percent CaO/MgO 2.33 to 5 wherein the glass composition has a log 2 viscosity in the range of about 2570° F. to about 2590° F. (1410° C. to 1421° C.) and a log 4 viscosity

  2. Claim 2Depends on #1

    The composition according to claim 1 , wherein CaO is in the range of greater than 9 to 12 weight percent.

  3. Claim 3Independent Claim

    The composition according to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
US 5,030,594 AHighly transparent, edge colored glass1991245
US 5,071,796 AFlat glass composition with improved melting and tempering properties199141
EP 0,555,552 A1Green-colored infrared and ultraviolet radiation absorbing glass and method of producing same—28
US 5,320,986 AGreen-colored infrared and ultraviolet radiation absorbing glass and method of producing same199440
US 5,344,798 ABlue-colored infrared and ultraviolet radiation absorbing glass and method of producing same199454
US 5,352,640 AColored glass compositions and glazings produced therewith199491
US 5,362,689 AInfrared and ultraviolet ray absorbing glass199453
US 5,364,820 ANeutral gray-colored infrared and ultraviolet radiation absorbing glass199463
US 5,380,685 ABronze-colored infrared and ultraviolet radiation absorbing glass199543
EP 0,653,385 A1Ultraviolet ray absorbent colored glass—16
US 5,545,596 AComposition for colored glass intended for the manufacture of glazing panes199678
JP H08217485 AUltraviolet absorbing glass—9
JP H08217486 AUltraviolet and infrared absorbing glass—8
US 5,558,942 AUltraviolet ray absorbent colored glass199657
EP 0,803,479 A1Dense green colored glass—31
US 5,688,727 AInfrared and ultraviolet radiation absorbing blue glass composition199781
US 5,700,579 AGlass compositions intended for the production of panes199733
EP 0,849,233 A1Ultraviolet and infrared radiation absorbing and low transmittance glass—34
US 5,780,372 AColored glass compositions199844
US 5,807,417 ANitrate-free method for manufacturing a blue glass composition199846
US 5,837,629 AGlass composition for making glazing1998104

Non-Patent Literature (2)

  • International Search Report mailed Dec. 3, 2002.
  • International Search Report mailed May 7, 2003.