Abstract
Raw materials for a copper alloy are melted in a high frequency smelter and cast, and milling, rolling, and annealing are carried out. Then, rolling is again carried out. Thereafter, the materials are heated at a temperature of 900° C. for one minute and are quenched in water, to be solution treated. Subsequently, the materials are heated at a temperature of 500° C. for five hours for aging, and then are cooled at a cooling rate in a range of 10 to 50° C. per hour until the materials are cooled to a temperature of 380° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a copper alloy, comprising the steps of: (a) melting and casting a raw material for said copper alloy, to form an alloy material; (b) solution treating said alloy material at a temperature in a range of 700 to 950° C.: (c) carrying out aging on said solution treated alloy material by heating said solution treated alloy material at a temperature in a range of 400 to 600° C. for two to eight hours; and (d) cooling said alloy material after said aging is carried out at a cooling rate in a range of 10 to 50° C. per hour until said alloy material is cooled to a temperature
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.