Copper-nickel-silicon-chromium alloy having improved electrical conductivity
Abstract
A copper-nickel-silicon-chromium alloy having a high hardness and improved electrical conductivity. The alloy is composed by weight of 2.0% to 3.0% nickel, 0.4% to 0.8% silicon, 0.1% to 0.5% chromium, and the balance copper. The silicon is used in excess of the stoichiometric relationship with nickel to provide excess silicon, and the chromium is used in excess of the stoichiometric relationship with the excess silicon. The alloy is heat treated by initially heating the alloy to a temperature in the range of 1600 DEG F. to 1800 DEG F. and is thereafter quenched. The quenched alloy is then subjected to a two-step aging treatment in which the alloy is initially aged at a temperature of 900 DEG F. to 1100 DEG F. to precipitate the metal silicides and develop a hardness in excess of 90 Rockwell B (185 Brinell) and subsequently is subjected to a second aging at a temperature in the range of 750 DEG F. to 900 DEG F., which serves to precipitate the excess chromium from solution and increase the electrical conductivity to a value greater than 45%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 30.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of heat treating a copper base alloy, consisting essentially by weight of 2.0% to 3.0% of a metal selected from the group consisting of nickel and cobalt and mixtures thereof, silicon in an amount slightly in excess of the stoichiometric amount necessary to form silicides of said metal, chromium in an amount in excess of the stoichiometric amount required to form chromium silicide with the excess silicon not combined as said metal silicides and the balance copper, comprising the steps of heating the alloy to a solution temperature, quenching the alloy, aging the alloy at a first aging
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 30 total)
References Cited — Backward Prior Art (4)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 1,658,186 A | Copper alloy and process of producing and treating the same | 1928 | 27 |
| US 1,763,303 A | Trolley wheel | 1930 | 3 |
| US 1,778,668 A | Electrode | 1930 | 12 |
| US 3,072,508 A | Method of heat treating copper base alloy | 1963 | 10 |