Patents
US 7,666,353 B2#3658571 Most CitedExpiredUnited States (USPTO)Utility

Aluminum-silicon alloy having reduced microporosity

22Forward Citations (#3658571 Global)
1.4/yrCitation Velocity (#4042615 Global)
3.88Citation PageRank (#5003002 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An aluminum silicon die cast alloy having a very low iron content and relatively high strontium content that prevents soldering to dies into die casting process. The alloys of the present invention also have a modified eutectic silicon and modified iron morphology, when iron is present, resulting in low microporosity and high impact properties. The alloy comprises 6-22% by weight silicon, 0.05 to 0.20% by weight strontium and the balance aluminum. Preferably, the alloy of the present invention contains in weight percent: 6-20% silicon, 0.05-0.10% strontium, 0.40% maximum iron and most preferably 0.20% maximum iron, 4.5% maximum copper, 0.50% maximum manganese, 0.60% maximum magnesium, 3.0% maximum zinc, balance aluminum. On cooling from the solution temperature, the strontium serves to modify the eutectic silicon structure as well as create an iron phase morphology change if iron is present, facilitating feeding through the aluminum interdendritic matrix. This, in turn, creates a finished die cast product with extremely low levels of microporosity defects. The strontium content also appears to create a non-wetting monolayer of strontium atoms on the surface of a molten casting, pre

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 22.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An aluminum silicon die cast alloy consisting essentially of: 7.80-11.5% by weight silicon, 0.05-0.10% by weight strontium, 0.40% by weight maximum iron, 4.5% by weight maximum copper, 0.50% by weight maximum manganese, 0.60% by weight maximum magnesium, 3.0% by weight maximum zinc, and the balance aluminum, wherein the alloy is free from grain refinement by titanium or boron, wherein the alloy avoids soldering to die casting dies, and wherein the alloy is formed by the step of die casting.

  2. Claim 2Depends on #1

    An aluminum silicon die cast alloy according to claim 1 , wherein the alloy has a hypoeutectic aluminum silicon microstructure.

  3. Claim 3Depends on #1

    An aluminum silicon die cast alloy according to claim 1 , wherein the alloy consists essentially of: 8.75-9.75% by weight silicon, 0.05-0.07% by weight strontium, 0.30% by weight maximum iron, 0.20% by weight maximum copper,

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Advanced Casting Research Center, Consortium Meeting, May 25, 2004," Report 04-#1, Metal Processing Institute.
  • "Aluminum and Aluminum Alloys" ASM Specialty Handbook, Copyright 1993.
  • "Aluminum and Aluminum Alloys", ASM International, 1993, p. 88-101.
  • "Aluminum Handbook," vol. 1: Fundamentals and Materials, First Edition, Aluminum-Verlag Marketing & Kommunikation GmbH, 1999.
  • "Aluminum Properties and Physical Metallurgy," American Society for Metals, Copyright 1984.