Abstract

A method and alloys for low pressure permanent mold casting without a coating are disclosed. The method includes preparing a permanent mold casting die that is devoid of die coating or lubrication along the die surface, preparing a permanent mold casting alloy, pushing the alloy into the die under low pressure, cooling the permanent mold casting, and removing the casting from the die. One alloy has 4.5-11.5% by weight silicon; 0.45% by weight maximum iron; 0.20-0.40% by weight manganese; 0.045-0.110% by weight strontium; 0.05-5.0% by weight copper; 0.01-0.70% by weight magnesium; and the balance aluminum. Another alloy has 4.2-5.0% by weight copper; 0.005-0.45% by weight iron; 0.20-0.50% by weight manganese; 0.15-0.35% by weight magnesium; 0.045-0.110% by weight strontium; 0.50% by weight maximum nickel; 0.10% by weight maximum silicon; 0.15-0.30% by weight titanium; 0.05% by weight maximum tin; 0.10% by weight maximum zinc; and the balance aluminum.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for low pressure permanent mold casting of metallic objects, the method comprising: preparing a permanent mold casting die, said die devoid of die coating or lubrication along a die casting surface; preparing a permanent mold casting alloy having 4.5-11.5% by weight silicon, 0.45% by weight maximum iron, 0.20-0.40% by weight manganese, 0.045-0.110% by weight strontium, 0.05-5% by weight copper, 0.10-0.7% by weight magnesium, and balance aluminum and wherein the alloy has a die soldering factor equivalent to or greater than 1.1, the die soldering factor defined as (10[Sr]+Mn+Fe); pushi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (5)

  • “Aluminum and Aluminum Alloys”, ASM Specialty Handbook, 1993, pp. 113-114.
  • “Designations and Chemical Composition Limits for Aluminum Alloys in the form of Castings and Ingots”, Aluminum Association, 2008.
  • Adam Kopper et al., Solder Resistance Mechanisms of Novel Al-Sr-Si Die Casting Alloys, Light Metals, Warrendale, PA, pp. 801-802, Coden: LMPMDF; ISSN:0147-, dated Jan. 1, 2006, XP009150752.
  • Elcee Group, Gravity Die Casting and Low Pressure Die Casting, dated Jun. 26, 2015, XP055477035, http://www.elcee.nl/wp-content/uploaded/2015/06, retrieved on May 22, 2018.
  • European Search Report, EP Patent Application No. 18163110.2, dated Aug. 3, 2018.