Method of manufacturing a silicon dioxide layer
Abstract
The invention relates to a of manufacturing a silicon dioxide layer of low roughness, that includes depositing a layer of silicon dioxide over a substrate by a low pressure chemical vapor deposition (LPCVD) process, the deposition process employing simultaneously a flow of tetraethylorthosilicate (TEOS) as the source material for the film deposition and a flow of a diluant gas that it not reactive with TEOS, so that the diluant gas/TEOS flow ratio is between 0.5 and 100; and annealing the silicon dioxide layer at a temperature between 600° C. and 1200° C., for a duration between 10 minutes and 6 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a composite substrate having a buried silicon dioxide layer which comprises: depositing a silicon dioxide layer on a source substrate by: depositing a layer of silicon dioxide upon the substrate using a low pressure chemical vapour deposition (LPCVD) process, wherein the layer is deposited employing simultaneously a flow of tetraethylorthosilicate (TEOS) as the source material for the film deposition and a flow of a diluent gas that is not reactive with TEOS, with the diluent gas and TEOS being present in the flow at a diluent gas/TEOS ratio of between about 0.5 and 1
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (21)
Non-Patent Literature (2)
- Chinese Search Report for application No. 200480044013.3.
- Pun, A.F., et al., "A method for reducing surface roughness during the thermal desorption of silicon". Thin Solid Films, 504 (2006) pp. 136-139.