Patents
US 7,446,019 B2#10828619 Most CitedActiveUnited States (USPTO)Utility

Method of reducing roughness of a thick insulating layer

10Forward Citations (#10828619 Global)
0.6/yrCitation Velocity (#14326673 Global)
1.57Citation PageRank (#21320131 Global)
6Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for reducing roughness of an exposed surface of an insulator layer on a substrate, by depositing an insulator layer on a substrate wherein the insulator layer includes an exposed rough surface opposite the substrate; treating the first substrate to form a zone of weakness beneath the insulator layer; and smoothing the exposed rough surface of the insulator layer by exposure to a gas plasma in a chamber. The chamber contains therein a gas at a pressure of greater than 0.25 Pa but less than 30 Pa, and the gas plasma is created using a radio frequency generator applying to the insulator layer a power density greater than 0.6 W/cm 2 but less than 10 W/cm 2 for at least 10 seconds to less than 200 seconds. Substrate bonding and layer transfer may be carried out subsequently to transfer the thin layer of substrate to the insulator layer and to a second substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 10.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for reducing roughness of an exposed surface of an insulator layer on a substrate, which comprises: depositing an insulator layer on a first substrate wherein the insulator layer comprises an exposed rough surface opposite the substrate; treating the first substrate to form a zone of weakness beneath the insulator layer; and smoothing the exposed rough surface of the insulator layer by exposure to a gas plasma in a chamber, wherein the chamber contains therein a gas at a pressure of greater than 0.25 Pa but less than 30 Pa, with the gas plasma created using a radiofrequency generator

  2. Claim 2Depends on #1

    The method of claim 1 wherein the gas pressure inside the chamber is in the range of 3Pa to 13 Pa.

  3. Claim 3Independent Claim

    The met

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • D. Pasquartello et al., "Surface Energy As A Function Of Self-Bias Voltage In Oxygen Plasma Wafer Bonding," Sensors and Actuators, vol. 82. pp. 239-244 (2000).
  • D.M. Hansen et al., "Chemical Role Of Oxygen Plasma In Wafer Bonding Using Borosilicate Glasses," Applied Physics Letters, vol. 79, No. 21, pp. 3413-3415 (2001).
  • D.M. Hansen et al., "Plasma Induced Chemical Changes at Silica Surfaces During Pre-Bonding Treatments", vol. 681E, Materials Research Society, pp. 12.2.1-12.2.6 (2001).
  • H. Moriceau et al., "Interest Of A Short Plasma Treatment To Achieve High Quality Si-SiO<SUB>2</SUB>-Si Bonded Structures," Abstract No. 1006, ECS (2003).