Method for producing a doped nitride film, doped oxide film and other doped films
Abstract
Adding at least one non-silicon precursor (such as a germanium precursor, a carbon precursor, etc.) during formation of a silicon nitride, silicon oxide, silicon oxynitride or silicon carbide film improves the deposition rate and/or makes possible tuning of properties of the film, such as tuning of the stress of the film. Also, in a doped silicon oxide or doped silicon nitride or other doped structure, the presence of the dopant may be used for measuring a signal associated with the dopant, as an etch-stop or otherwise for achieving control during etching.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a doped silicon nitride film, doped silicon oxide film, doped silicon oxynitride film or doped silicon carbide film, comprising: providing at least one silicon precursor, in the case of a doped silicon nitride film, doped silicon oxide film or doped silicon oxynitride film, providing at least one nitrogen precursor or an oxygen precursor; providing at least one non-silicon precursor selected from the group consisting of an aluminum precursor, a hafnium precursor, and an indium precursor; and forming a doped silicon nitride film, a doped silicon oxide film, a doped silico
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (26)
Non-Patent Literature (1)
- EerNisse, "Stress in ion-implanted CVD Si3N4 Films", J. Applied Physics, Aug. 1997, vol. 48, No. 8, pp. 3337-3341.