Method for fabricating semiconductor device
Abstract
Ions are implanted into a silicon nitride film at a dose of not more than 1×10 15 cm -2 so that the projected range of the ions is 20 to 60% of the thickness of the silicon nitride film. This enables the stress of the nitride film to be reduced while enjoying good productivity without introduction of defects into a silicon substrate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 11.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for fabricating a semiconductor device, comprising the steps in sequence of: forming a pad oxide film and a silicon nitride film successively on a semiconductor substrate; implanting ions having a mass number of at least 14, by means of a beam directed normal to the substrate, into said silicon nitride film; selectively removing said silicon nitride film in accordance with a field pattern; growing silicon oxide films at positions where said silicon nitride film is removed; removing said pad oxide film and said silicon nitride film which is left at the step of selectively remov
- Claim 2Depends on #1
The method according to claim 1, wherein the projected range of ions implanted into the silicon nitride film is 20 to 60% of the thickne
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (5)
- Journal of Applied Physics, vol. 48, No. 8 (1977) by E.P. EerNisse pp. 3337 3341.
- Journal of Applied Physics, vol. 48, No. 8 (1977) by E.P. EerNisse pp. 3337-3341.
- Published Sendia Laboratories, Albequerque, NM Apr. 15, 1997.
- Published--Sendia Laboratories, Albequerque, NM Apr. 15, 1997.
- Stress in ion implanted CVD Si 3 N 4 films Author E.P. EerNisse.