Patents
US 7,592,619 B2#7754262 Most CitedActiveUnited States (USPTO)Utility

Epitaxy layer and method of forming the same

13Forward Citations (#7754262 Global)
0.8/yrCitation Velocity (#9812876 Global)
2.07Citation PageRank (#13778453 Global)
14Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming an epitaxial layer of uniform thickness is provided to improve surface flatness. A substrate is first provided and a Si base layer is then formed on the substrate by epitaxy. A Si—Ge layer containing 5 to 10% germanium is formed on the Si base layer by epitaxy to normalize the overall thickness of the Si base layer and the Si—Ge layer containing 5 to 10% germanium.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An epitaxy layer of uniform thickness, comprising: a Si base substrate; a first epitaxial Si—Ge layer containing more than 20% germanium on the Si base substrate; and a second epitaxial Si—Ge layer containing 5-10% germanium, disposed directly on the first epitaxial Si—Ge layer to normalize an overall thickness of the first epitaxial Si—Ge layer and the second epitaxial Si—Ge layer.

  2. Claim 2Depends on #1

    The epitaxy layer according to claim 1 , wherein the second epitaxial Si—Ge layer containing 5-8% germanium.

  3. Claim 3Depends on #1

    The epitaxy layer according to claim 1 , wherein the thickness of the first wavy epitaxial Si—Ge layer is about 50-500 Å.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗