A method of fabricating a semiconductor structure. According to one aspect of the invention, on a first semiconductor substrate, a first compositionally graded Si 1-x Ge x buffer is deposited where the Ge composition x is increasing from about zero to a value less than about 20%. Then a first etch-stop Si 1-y Ge y layer is deposited where the Ge composition y is larger than about 20% so that the layer is an effective etch-stop. A second etch-stop layer of strained Si is then grown. The deposited layer is bonded to a second substrate. After that the first substrate is removed to release said first etch-stop Si 1-y Ge y layer. The remaining structure is then removed in another step to release the second etch-stop layer. According to another aspect of the invention, a semiconductor structure is provided. The structure has a layer in which semiconductor devices are to be formed. The semiconductor structure includes a substrate, an insulating layer, a relaxed SiGe layer where the Ge composition is larger than approximately 15%, and a device layer selected from a group consisting of, but not limited to, strained-Si, relaxed Si 1-y Ge y layer, strained S 1-z Ge z layer, Ge, GaAs, III-V ma

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 47.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor structure that includes a monocrystalline semiconductor substrate, said semiconductor structure comprising: a first compositionally graded Si 1-x Ge x buffer where x increases from about zero to a value less than about 0.2; a uniform Si 1-y Ge y layer where y is larger than about 0.2; and a second compositionally graded Si 1-z Ge z buffer where z decreases from about 0.2 to a value less tan 0.2.

  2. Claim 2Independent Claim

    A semiconductor etch-stop layer structure comprising: a monocrystalline semiconductor substrate; a compositionally graded Si 1-x G x buffer where x increases from about zero to a value less than about 0.2; a first etch-stop Si 1-y Ge y layer where y is larger than about 0.2; a second etch-stop layer of strained Si; and between said first and second etch-stop layers, one or more material layers selected from the group consisting

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 47 total)

PatentTitleYearCitations
US 7,517,465 B2Ultra lightweight photovoltaic device and method for its manufacture20093
US 2008233725 A1Methods for stressing semiconductor material structures to improve electron and/or hole mobility of transistor channels fabricated therefrom, and semiconductor devices including such structures—7
US 2017317103 A1Integrated circuits with selectively strained device regions and methods for fabricating same—0
US 7,304,328 B2Use of hydrogen implantation to improve material properties of silicon-germanium-on-insulator material made by thermal diffusion20075
US 7,473,587 B2High-quality SGOI by oxidation near the alloy melting temperature20096
US 7,902,046 B2Thin buffer layers for SiGe growth on mismatched substrates20113
US 7,923,350 B2Method of manufacturing a semiconductor device including etching to etch stop regions20118
US 7,592,619 B2Epitaxy layer and method of forming the same200913
US 7,759,233 B2Methods for stressing semiconductor material structures to improve electron and/or hole mobility of transistor channels fabricated therefrom, and semiconductor devices including such structures20107
US 8,367,521 B2Manufacture of thin silicon-on-insulator (SOI) structures20137
US 7,425,751 B2Method to reduce junction leakage current in strained silicon on silicon-germanium devices200811
US 2005130361 A1Method to reduce junction leakage current in strained silicon on silicon-germanium devices—9
US 8,227,792 B2Relaxed low-defect SGOI for strained SI CMOS applications20122
US 11,049,797 B2Method for manufacturing a semiconductor structure comprising a semiconductor device layer formed on a tem, porary substrate having a graded SiGe etch stop layer therebetween20210
US 2008277734 A1Implantation processes for straining transistor channels of semiconductor device structures and semiconductor devices with strained transistor channels—16