Patents
US 7,556,840 B2#27144286 Most CitedActiveUnited States (USPTO)Utility

Coating using metal organic chemical vapor deposition

4Forward Citations (#27144286 Global)
0.2/yrCitation Velocity (#30581182 Global)
1.09Citation PageRank (#36845204 Global)
17Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method is provided for applying a coating over a substrate surface of an engine component. The method includes inserting the engine component within a deposition chamber, heating the deposition chamber to a temperature between 325° C. and 500° C., supplying one or more precursors to the heated deposition chamber, subjecting the engine component to the one or more precursors for about five hours to form an inert oxide layer over the substrate surface of the engine component having a thickness of approximately 1-5 microns.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of applying one or more inert oxide layers on at least one substrate surface comprising: disposing the substrate surface within a deposition chamber; heating the deposition chamber to a temperature of approximately 325° C.; supplying one or more precursors to the deposition chamber at approximately 325° C.; subjecting the substrate surface to the one or more precursors at approximately 325° C. for about two hours; halting the application of one or more precursors; heating the deposition chamber to a temperature of approximately 375° C.; supplying one or more precursors to the depositi

  2. Claim 2Depends on #1

    The method of claim 1 , further including: forming the inert oxide layer

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
US 5,077,091 ADeposition process in the vapour phase at low temperature of a ceramic coating of the metallic nitride or carbonitride type199121
EP 0,504,959 A2Carbon-alloyed cubic boron nitride films—11
US 5,330,611 ACubic boron nitride carbide films199430
US 5,336,324 AApparatus for depositing a coating on a substrate1994114
US 5,453,494 AMetal complex source reagents for MOCVD1995265
US 5,544,618 AApparatus for depositing a coating on a substrate199623
JP H09143684 AMetallic film coated high molecular article and its manufacture—4
US 5,780,110 AMethod for manufacturing thermal barrier coated articles199867
US 6,066,196 AMethod for the chemical vapor deposition of copper-based films and copper source precursors for the same200082
WO 0,047,404 A1Chemical vapor deposition of tungsten nitride—25
US 6,245,435 B1Decorative corrosion and abrasion resistant coating200145
US 6,495,271 B1Spallation-resistant protective layer on high performance alloys200230
US 6,521,294 B2Aluminiding of a metallic surface using an aluminum-modified maskant, and aluminum-modified maskant200319
US 6,723,186 B2Method of manufacturing metallic film consisting of giant single crystal grains200410
US 6,777,327 B2Method of barrier metal surface treatment prior to Cu deposition to improve adhesion and trench filling characteristics20042
US 6,849,241 B2Device and method for depositing one or more layers on a substrate200553
US 6,884,466 B2Process for low-temperature metal-organic chemical vapor deposition of tungsten nitride and tungsten nitride films200546