Patents
US 6,884,466 B2#1108658 Most CitedExpiredUnited States (USPTO)Utility

Process for low-temperature metal-organic chemical vapor deposition of tungsten nitride and tungsten nitride films

46Forward Citations (#1108658 Global)
2.2/yrCitation Velocity (#1725721 Global)
3.36Citation PageRank (#6301057 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Processes for producing tungsten nitride and tungsten nitride films are provided in which a tungsten carbonyl compound and a nitrogen-containing reactant gas are reacted at a temperature below about 600° C. Tungsten nitride precursors are also included which comprise a tungsten carbonyl compound capable of forming a tungsten nitride film in the presence of a nitrogen-containing reactant gas at a temperature of less than about 600° C. A process for forming a film by atomic layer deposition is also provided which includes introducing a substrate having a surface into a deposition chamber and heating the substrate to a temperature sufficient to allow adsorption of a tungsten source precursor or an intermediate thereof, and thereafter sequentially introducing by pulsing: a tungsten source precursor which is absorbed as a monolayer, a purging inert gas, a nitrogen-containing gas for reacting with the monolayer to form a first tungsten nitride layer on the substrate surface, and an inert purging gas, and repeating the sequence to form a film of desired thickness.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 46.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the production of tungsten nitride comprising reacting a tungsten carbonyl compound with a nitrogen-containing gas in a deposition chamber at a temperature below about 600° C., wherein the tungsten carbonyl compound is introduced into the chamber in a vapor state separately from the introduction of the nitrogen-containing gas prior to reacting the tungsten carbonyl compound and the nitrogen-containing gas.

  2. Claim 2Depends on #1

    A process for the production of tungsten nitride according to claim 1 , wherein the nitrogen-containing gas is ammonia.

  3. Claim 3Depends on #1

    The process for the production of tungsten nitride according to claim 1 , wherein the tungsten nitride has a formula WN x , wherein 0.1≦x≦2.0.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • A. Jain, et al., "Selective and blanket copper chemical vapor deposition for ultra-large-scale integration", J. Vac. Sci. Technol. B., vol. 11, No. 6 (1993), pp. 2107-2113.
  • A. Jain, et al., "Selective CVD of Copper on Tungsten Versus SiO<SUB>2 </SUB>from (B-diketonate) CuL<SUB>n </SUB>Copper (1) Precursors Via SiO<SUB>2 </SUB>Surface Modification," Conference Proc. ULSI-VIII (1993) Materials Research Society, pp. 83-89.
  • D. Ugolini et al., "Photoelectron Spectroscopy studies of chemical vapor deposition of Ta from a TaF5 precursor on Si and SiO<SUB>2 </SUB>substrates", J. Appl. Phys. vol. 70 (1991), pp. 3899-3906.
  • H.O.Pierson, Handbook of Chemical Vapor Deposition, (1992), pp. 98-102, 246-247.
  • Klaus, J.W., et al., "Atomic layer deposition of tungsten and tungsten nitride using sequential surface reactions," AVS 46.sup.th International Symposium, Seattle, WA, abstract TF-TuM6 (1999) (no month avail.).*