Anode active material, manufacturing method thereof, and non-aqueous electrolyte secondary battery

36Forward Citations (#1707983 Global)
2.1/yrCitation Velocity (#1837179 Global)
3.19Citation PageRank (#6851689 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In order to provide a 3V level non-aqueous electrolyte secondary battery with a flat voltage and excellent cycle life at a high rate with low cost, the present invention provides a positive electrode represented by the formula: Li2±alpha[Me]4O8-x, wherein 0<=alpha<0.4, 0<=x<2, and Me is a transition metal containing Mn and at least one selected from the group consisting of Ni, Cr, Fe, Co and Cu, said active material exhibiting topotactic two-phase reactions during charge and discharge.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 36.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A positive electrode active material represented by the composition formula: Li 2±α [Me] 4 O 8−x , wherein 0≦α<0.4, 0≦x<2, and Me is a transition metal containing Mn and at least one selected from the group consisting of Ni, Cr, Fe, Co and Cu, said active material exhibiting first and second topotactic two-phase reactions respectively during first and second stages of charge and discharge, and characterized in that the phase of the transition metal has a 2×2 superlattice.

  2. Claim 2Depends on #1

    The positive electrode active material in accordance with claim 1 , characterized in that the ratio between Mn and other transition metal is substantially 3:1.

  3. Claim 3Depends on #1

    The positive electrode active material in accordance with claim 1 , characterized in that said positive electrode active material has a spinel-framework-structure and

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 36 total)

Non-Patent Literature (5)

  • "Solid-State Redox Reactions of LiNi1/2Co1/2O2 (R3m) for 4 Volt Secondary Lithium Cells", Ueda et al., J. Electrochem Soc., vol. 141, No. 8, Aug. 1994 (C) The Electrochemical Society, Inc. pp. 2011-2014.
  • “Solid-State Redox Reactions of LiNi1/2Co1/2O2 (R3m) for 4 Volt Secondary Lithium Cells”, Ueda et al., J. Electrochem Soc., vol. 141, No. 8, Aug. 1994 © The Electrochemical Society, Inc. pp. 2011-2014.
  • Abraham, et al., "Surface changes on LiNi0.8Co0.2O2 particles during testing of high power lithium-ion cells," Electrochemistry Communications, May 2002, p. 620-625, vol. 4, Elsevier.
  • Amine et al., A New Three-Volt Spinel Li1+xMn1.5Ni0.5O4 for Secondary Lithium Batteries, J. of Electrochem. Soc., vol. 143, No. 5, p. 1607-1613. May 1996.
  • Ariyoshi, Kingo et al., "Topotactic Two-Phase Reactions of Li[Ni1/2MN3/2] O4 (P4332) in Nonaqueous Lithium Cells," Journal of the Electrochemistry Society, vol. 151, No. 2, 2004, pp. A296-A303, XP-002502626.