Patents
US 5,264,201 A#31098 Most CitedExpiredUnited States (USPTO)Utility

Lithiated nickel dioxide and secondary cells prepared therefrom

255Forward Citations (#31098 Global)
7.7/yrCitation Velocity (#94860 Global)
93.22Citation PageRank (#23806 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Lithiated nickel dioxide cathode-active materials for electrochemical cellsaving the formula Li x Ni 2-x-y M y O 2 , with x being between about 0.8 and about 1.0, M being one or more metals selected from cobalt, iron, chromium, titanium, manganese and vanadium, and y being less than about 0.2, with the proviso that y is less than about 0.5 for cobalt, which material is substantially free of lithium hydroxide and lithium carbonate. The materials are prepared by providing a substantially homogeneous dry intermediate mixture of a starting material containing a nickel compound selected from nickel oxide, nickel hydroxide, and mixtures thereof, and optionally including one or more oxides or hydroxides of a transition metal selected from cobalt, iron, chromium, titanium, manganese and vanadium, together with between about a 10 and about a 25% stoichiometric excess of lithium hydroxide. The mixture is heat treated at a temperature above about 600° C. in an atmosphere substantially free of carbon dioxide and having a partial pressure ratio of oxygen to water vapor greater than about 15, after which any lithium hydroxide or lithium carbonate present in the mixture is removed. Thermally stab

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 255.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a lithiated nickel dioxide cathode-active material for an electrochemical cell, having a formula Li x Ni 2-x-y M y O 2 , wherein x is between about 0.8 and about 1.0, M is one or more metals selected from the group consisting of cobalt, iron, titanium, manganese, chromium and vanadium, and y is less than about 0.2, with the proviso that y is less than about 0.5 for cobalt, which material is substantially free of lithium hydroxide and lithium carbonate, said method comprising the steps of: providing a substantially homogeneous dry intermediate mixture of a starting materia

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Bronger et al., Z. Anorg. Allg. Chem., 333, 188 200 (1956).
  • Bronger et al., Z. Anorg. Allg. Chem., 333, 188-200 (1956).
  • Dyer et al., JACS, 76, 1499 1503 (1954).
  • Dyer et al., JACS, 76, 1499-1503 (1954).
  • Fensham, JACS, 76, 969 71 (1954).