Patents
US 7,524,533 B2#22448197 Most CitedExpiredUnited States (USPTO)Utility

Diffusion barrier layers and processes for depositing metal films thereupon by CVD or ALD processes

5Forward Citations (#22448197 Global)
0.3/yrCitation Velocity (#26454840 Global)
1.11Citation PageRank (#36223996 Global)
24Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process is described for depositing a metal film on a substrate surface having a diffusion barrier layer deposited thereupon. In one embodiment, the process includes: providing a surface of the diffusion barrier layer that is substantially free of an elemental metal and forming the metal film on at least a portion of the surface via deposition by using a organometallic precursor. In certain embodiments, the surface of the diffusion barrier layer may be exposed to an adhesion promoting agent prior to or during at least a portion of the forming step. Suitable adhesion promoting agents include nitrogen, nitrogen-containing compounds, carbon-containing compounds, carbon and nitrogen containing compounds, silicon-containing compounds, silicon and carbon containing compounds, silicon, carbon, and nitrogen containing compounds, and mixtures thereof. The process of the present invention provides substrates having enhanced adhesion between the diffusion barrier layer and the metal film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 5.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for forming a metal film on at least one surface of a diffusion barrier layer comprising tungsten nitride, the process comprising: providing at least one surface of the diffusion barrier layer wherein the at least one surface comprises a stoichiometric amount or greater of nitrogen relative to tungsten contained therein and wherein the at least one surface is comprised of an orientation selected from the group consisting of a (111) preferred orientation and a (100) preferred orientation; and forming the metal film via a chemical vapor deposition process on the at least one surface us

  2. Claim 2Depends on #1

    The process of claim 1 wherein the at least one surface is comprised of non-stoichiometric tungsten nitride having a greater amount of nitrogen atoms than tungsten atoms contained therein.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
JP S60258471 AFormation of tungsten-aluminum alloy film—3
US 5,019,531 AProcess for selectively growing thin metallic film of copper or gold1991118
US 5,085,731 AVolatile liquid precursors for the chemical vapor deposition of copper1992117
US 5,242,860 AMethod for the formation of tin barrier layer with preferential (111) crystallographic orientation199390
US 5,434,044 AMethod for the formation of tin barrier layer with preferential (111) crystallographic orientation199533
JP H08127870 AFormation of thin titanium nitride film—14
US 5,521,120 AMethod for the formation of tin barrier layer with preferential (111) crystallographic orientation199630
EP 0,818,559 A2Chamber for constructing a film on a semiconductor wafer—15
WO 9,900,830 A1Improved deposition of tungsten nitride using plasma pretreatment in a chemical vapor deposition chamber—9
JP 2000219968 ARAW MATERIAL FOR Cu-CVD PROCESS AND Cu-CVD DEVICE—9
EP 1,029,943 A1Process for producing barrier film—4
US 6,150,268 ABarrier materials for metal interconnect200011
WO 0,071,550 A1Copper source reagent compositions, and method of making and using same for microelectronic device structures—10
US 6,165,555 AMethod for forming copper film using chemical vapor deposition200029
EP 1,142,894 A2Volatile precursors for deposition of metals and metal-containing films—13
US 6,334,249 B2Cavity-filling method for reducing surface topography and roughness200225
US 2002043468 A1Seed repair and electroplating bath—20
US 6,413,864 B1Method of manufacturing a copper metal wiring in a semiconductor device200244
US 6,423,201 B1Method of improving the adhesion of copper200224
US 6,509,266 B1Halogen addition for improved adhesion of CVD copper to barrier200312
US 6,545,357 B2Metal nitride barrier layer and electroplating seed layer with the same metal as the metal nitride layer200322
US 6,955,986 B2Atomic layer deposition methods for forming a multi-layer adhesion-barrier layer for integrated circuits200543
US 7,018,917 B2Multilayer metallization200621
US 7,311,946 B2Methods for depositing metal films on diffusion barrier layers by CVD or ALD processes200712

Non-Patent Literature (5)

  • A. Bouteville, et al., "Low Temperature Rapid Thermal Low Pressure Chemical Vapor Deposition of (111) Oriented TiN Layers from the TiCI4-NH3-H2 Gaseous Phase," Microelectronic Engineering 37/38, pp. 421-425 (1997).
  • A. V. Gelatos, et al., "Chemical Vapor Deposition of Copper from Copper+1 Precursors in the Presence of Water Vapor," Appl. Phys. Lett. 63 (20), pp. 2842-2844 (1993).
  • B. H. Weiller, "CVD of Titanium Nitride for Electronic Applications: Gas Phase Chemical Kinetics for Fundamental Principles and Modeling," Electrochemical Society Proceedings, vol. 96(5), pp. 231-238.
  • B. Mehrotra, et al., "Properties of Direct Current Magnetron Reactively Sputtered TaN," J. Vac. Sci. Technol. B5 (6), pp. 1736-1740 (1987).
  • E. S. Hwang, et al., "Surfactant-Catalyzed Chemical Vapor Deposition of Copper Thin Films," Chem Mater. 12, pp. 2076-2081 (2000).