Patents
US 6,334,249 B2#3044706 Most CitedExpiredUnited States (USPTO)Utility

Cavity-filling method for reducing surface topography and roughness

25Forward Citations (#3044706 Global)
1.0/yrCitation Velocity (#6134805 Global)
3.68Citation PageRank (#5449456 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of minimizing the volume of the depressions 240 in aluminum cavity filling processes, by-depositing a conformal first layer of aluminum alloy 220 by chemical vapor deposition, long-throw sputtering, collimated sputtering, or ionized physical vapor deposition, to partially fill the cavity 202 . This layer is preferably deposited at low temperature (eg. less than 300 degrees C.) and lower deposition pressure (if deposited by sputtering). Subsequently, a second layer of aluminum alloy 230 is deposited by sputtering at temperatures greater than 350 degrees C. and at high power (e.g. greater than 10 kW) to close the mouth of cavity 202 . The second layer of aluminum 230 is then forced into the remaining volume of the cavity 202 . As part of the cavity 202 is filled with aluminum, alloy 220 before the high pressure aluminum extrusion/reflow, less material is required to be transported into the cavity 202 . Therefore, a smaller depression 240 above the cavity is produced. This method is particularly advantageous in multi-level interconnect applications involving aluminum cavity filling.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 25.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming an integrated circuit metallization layer which fills an opening in a dielectric layer, comprising the steps of; forming said opening in said dielectric layer, after forming said opening, depositing an adhesion layer in said opening; depositing a conductive layer predominantly comprising aluminum to fill at least 10 percent of a volume of said opening; depositing a metal layer predominantly comprising aluminum over said conductive layer and over the dielectric layer; and extruding said metal layer into said opening under high pressure.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said opening has a height to width ratio of at least 3:1.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein said conductive layer is deposited at a temperature less than 300 degrees C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • "A Prcocess to Incorporate CVD TiN as Barriers for Quarter Micron Contacts With High Pressure Extruded Al Alloy", pp. 1-7 (Wei-Yung Hsu, Girish Dixit, Jiong-Ping Lu, Qi-Zhong Hong, Anthony Konecni, J.D. Luttmer, and R.H, Havemann).
  • 1996 IEEE, "A Novel Low Temperature PVD Planarized Al-Cu Process for High Aspect Ratio Sub-Half Micron Interconnect", pp. 14.2.1-14.2.4 (B. Zhao, M.A. Biberger, V. Hoffman, S.Q. Wang, P.K. Vasudev, and T.E. Seidel).
  • Jun. 27-29, 1995 VMIC Conference, "A Multilevel Al-Plug Technology for Sub-Half Micron Metallization", pp. 537-543 (P.J. Holverson, C.D. Dobson, Paul Rich, D.C. Butler, G.R. Green, M.G.M. Harris and Arthur McGeown, G.A. Dixit. S. Poarch, K. Hamamoto, B. Bohannon, W.Y. Hsu and R.H. Havemann).
  • Mat. Res. Soc. Symp. Proc. vol. 354, 1995 Materials Research Society, "Directional Sputter Deposition for Semiconductor Applications", pp. 503-510 (S.M. Rossnagel).