Manufacturing method for friction welded aluminum alloy parts
Abstract
A method for manufacturing aluminium alloy parts with precipitation hardening including friction stir welding of at least two elements made from the same alloy or different alloys, solution heat treatment, and quenching of welded parts, in which the elements are subjected to heat treatment before welding at temperature T for at least 2t 1 , t 1 being defined as the minimum treatment duration at temperature T leading to a specific melting peak energy defined by AED equal to less than 1 J/g. A method according to the invention substantially avoids an increase in the grain size following solution heat treatment after welding. The invention further relates to novel aluminum materials as well as uses therefor.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 9.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for manufacturing aluminum alloy parts with precipitation hardening comprising: subjecting at least two elements made from the same alloy or different alloys to heat treatment at a temperature T for at least 2t 1 ,wherein t 1 comprises a minimum treatment duration at temperature T leading to a specific melting peak energy defined by Differential Scanning Calorimetry of less than 1 J/g, and wherein the treatment duration is at least 72 hours; after said heat treatment, friction stir welding said at least two elements; and thereafter conducting a solution heat treatment, and quenching
- Claim 2Depends on #1
A method according to claim 1 , wherein the specific melting peak energy is less than 0.5 J/g.
- Claim 3Depends on #2
A method according to claim 2 , wherein the specific melting peak energy is less than 0.1 J/g.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (1)
- Hassan et al, "Stability of Nugget Zone Grain Structures in High-Strength Al-alloy Friction Stir Welds During Solution Treatment", Acta Materialia vol. 51, 2003, pp. 1923-1936.