Method of producing a high strength balanced Al-Mg-Si alloy and a weldable product of that alloy
Abstract
The present invention relates to a method for producing high strength balanced Al—Mg—Si alloy with an improved fatigue crack growth resistance and a low amount of intermetallics, comprising the steps of a) casting an ingot with the following composition (in weight percent) Si: 0.75–1.3, Cu: 0.6–1.1, Mn: 0.2–0.8, Mg: 0.45–0.95, Fe: 0.01–0.3, Zr: <0.25, Cr: <0.25, Zn: <0.35, Ti: <0.25, impurities each less than 0.05 and less than 0.20 in total, balance aluminum, b) optional homogenization of the cast ingot, c) pre-heating the ingot after casting for 4 to 30 hours with temperatures above 520° C., d) hot working the ingot and optionally cold working, e) solution heat treating, and f) quenching the worked product. The pre-heating is preferably performed for 6 to 18 hours with temperatures between 530° C. and 560° C. The alloy has a fatigue crack growth rate at ΔK=20 MPa√m of below 9.0E−04 and at ΔK=40 MPa√m of below 9.0E−03, wherein the amount of intermetallics within the finally worked alloy product, according to the measured specific energy Delta H associated with the DSC signal, is below 1.5 J/g.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 25.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Method of producing a high-strength balanced Al—Mg—Si alloy product with an improved fatigue crack growth resistance and a low amount of intermetallics, comprising the steps of: a) casting an ingot with the following composition (in weight percent): Si: 0.75+14 1.3+11 Cu: 0.6+14 1.1 Mn: 0.2+14 0.8 Mg: 0.45+14 0.95 Fe: 0.01+14 0.3+11 Zr: +21 0.25 Cr: +21 0.25 Zn: +21 0.35 Ti: +21 0.25 V: +21 0.25 Hf: +21 0.25 impurities each less than 0.05 and less than 0.20 in total, balance aluminum, b) hom
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 25 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (1)
- "Aluminum and Aluminum Alloys" ASM Internaitonal, 1993, pp 22-23,45.