Patents
US 7,442,264 B2#97381555 Most CitedExpiredUnited States (USPTO)Utility

Method of using low alloy anticoking steels with an increased silicon and manganese content in refining and petrochemicals applications

0Forward Citations (#97381555 Global)
0.0/yrCitation Velocity (#97381555 Global)
0.56Citation PageRank (#97381555 Global)
22Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The use is described, in the fabrication of apparatus and equipment used in refining and in petrochemicals (for example furnace, reactor or line elements), of a steel composition comprising: at most 0.25% C; more than 1% up to 10% Mn; 1.5% to 5% Si; at most 0.03% P; at most 0.03% S; 4% to 10% Cr; 0.5% to 2% Mo; at most 0.40% V; and at most 0.10% N; the complement to 100% being essentially iron. Steels comprising: at most 0.15% C; more than 2% up to 10% Mn; 1.5% to 5% Si; at most 0.03% P; at most 0.03% S; 4% to 10% Cr; more than 0.5% up to 2% Mo; at most 0.40% V; and at most 0.10% N; the complement to 100% being essentially iron; are themselves novel.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    5% to 5% Si; at most 0.03% P; at most 0.03% S; 4% to 10% Cr; 0.5% to 2% Mo; at most 0.40% V; and at most 0.10% N; the complement to 100% being essentially iron, and with the provision that the alloy has an Mn/Si ratio in the range of 1.5/1 to 3/1, wherein said alloy exhibits anticoking properties.

  2. Claim 2Depends on #1

    A process according to claim 1 , wherein said furnace, reactor or tube is fabricated as a bulk piec

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (22)

PatentTitleYearCitations
GB 419,009 AImprovements in the manufacture of articles from steel alloys—2
GB 517,118 AImprovements in and relating to improved steels and the application thereof—12
GB 1,220,620 AWearing member having a hard surfacing layer high in wear-resistance and heat crack-proofness—9
US 3,674,468 AHigh-strength silicon steel19727
US 3,847,600 AHigh temperature alloy steel197413
US 3,929,428 AWearing member having a pad-welded surface layer high in wear-resistance and heat crack-resistance19758
DE 2,701,565 A1Abrasion resistant steel - for scraper teeth of earth moving machine esp. bulldozer—3
US 4,129,442 AWear- and impact-resisting cast steel19788
US 4,721,600 ASuperplastic ferrous duplex-phase alloy and a hot working method therefor198826
EP 0,338,133 A2Steels for hot working press tools—15
JP H02254135 ASteel for hot press tool—6
US 5,011,656 ASteels for hot working press tools19917
JP H046247 ASteel for waste incineration furnace boiler—11
US 5,278,881 AFe-Cr-Mn Alloy199417
EP 0,718,415 A1Anti-coking steels—5
US 5,665,669 AMetallic honeycomb body for supporting catalyst and production method thereof199711
US 5,693,155 AProcess for using anti-coking steels for diminishing coking in a petrochemical process199716
FR 2,776,671 A1Aciers faiblement allies anti-cokage—2
US 6,235,238 B1Apparatus comprising furnaces, reactors or conduits having internal walls comprising at least partly of a steel alloy200110
EP 1,223,230 A1Use of austenitic stainless steel for applications requiring anti-coking properties—9
US 2002129876 A1Use of austenitic stainless steels in applications requiring anti-coking properties—5
US 6,749,894 B2Corrosion-resistant coatings for steel tubes200436