Process for using anti-coking steels for diminishing coking in a petrochemical process
Abstract
For diminishing coking in a petrochemical process, coking-resistant steel containing by weight: about 0.05% to 0.06% of carbon; about 2.5% to 5% of silicon; 10% to 20% of chromium; 10% to 15% of nickel 0.5% to 1.5% of manganese; 0-0.5% of titanium; at most 0.8% of aluminium; the complement to 100% being essentially iron, can be used to manufacture tubes and plates for producing reactors or elements thereof, as well as for coatings of the internal walls of furnaces, reactors or tubings where coking can occur.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 16.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for diminishing coking in a petrochemical process carried out at temperatures of between 350° C. and 1100° C. in contact with a surface subjectable to coking, comprising providing said surface at least in part, with a steel consisting essentially of, by weight: about 0.05% to about 0.06% of carbon; 2.5% to 5% of silicon; 10% to 20% of chromium; 10% to 15% of nickel 0.5% to 1.5% of manganese: at most 0.8% of aluminum; 0 to 0.5% of titanium; the complement to 100% being iron, thereby diminishing said coking compared to surfaces made from other steels.
- Claim 2Depends on #1
A process according to claim 1, wherein the steel contains 0.25% to about 0.5% by weight of titanium.
- Claim 3Depends on #1
A process according to claim 1, wherein the steel consists essentially of the following composition by weight: about 0.06% of carbon; about
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 16 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (2)
- Abstract, JP 2 156049, Jun. 15, 1990.
- Abstract, JP 2-156049, Jun. 15, 1990.