Data storage medium and method for the preparation thereof
Abstract
A data storage medium includes a substrate, a reflective metal layer, and a haze-prevention layer between the substrate and the reflective metal layer. The substrate includes an amorphous thermoplastic resin having a heat distortion temperature of at least about 140° C., a density less than 1.7 grams per milliliter, and an organic volatiles content less than 1,000 parts per million measured according to ASTM D4526. The haze-prevention layer includes a material having a volume resistivity of at least 1x10<SUP>-4 </SUP>ohm-centimeters and a tensile modulus of at least about 3x10<SUP>5 </SUP>pounds per square inch. The data storage medium resists hazing of the reflective layer at elevated temperatures.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A data storage medium, comprising: a substrate comprising an amorphous thermoplastic resin having a heat distortion temperature of at least about 140° C. measured at 66 pounds per square inch according to ASTM D648. a density less than 1.7 grams per milliliter, and an orannic volatiles content less than 1,000 parts per million measured according to ASTM D4526; a reflective metal layer; a haze-prevention layer interposed between the substrate and the reflective metal layer, wherein the haze-prevention layer comprises a material having a volume resistivity of at least 1×10 −4 ohm-centimeters me
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- ASTM D 1003-00 Standard Test Method for Haze and Luminous Transmittance of Transparent Plastics (6 pages).
- ASTM D 523-89 (Reapproved 1999) Standard Test Method for Specular Gloss (5 pages).
- http://www.matweb.com/reference/deflection-temperature.asp (2 pgs).
- Human Translation of JP58196636; Publication Date Nov. 16, 1983; 4 pages.
- JP2523303B2; Aug. 7, 1996; Machine Translation Only (19 pages).