Patents
US 4,156,069 A#22934 Most CitedExpiredUnited States (USPTO)Utility

Bisphenol-A/terephthalate/carbonate melt processable copolymers

293Forward Citations (#22934 Global)
6.2/yrCitation Velocity (#162955 Global)
22.63Citation PageRank (#271610 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Copolymers consisting of bisphenol-A ("BPA"), terephthalate ("TP"), and carbonate moieties in mol ratio from 2:0.8:1.2 to 2:1.3:0.7, which are melt processable in the sense of (a) showing no more than 10% change in viscosity number upon compression molding for 10 minutes at 320 DEG C. to form a plaque, (b) developing, in 2% (gm./ml.) DCM solution, a "yellowness index" of no more than 10 as observed by ASTM Test No. D-1925, using a 2 cm. path length; which copolymers approximate in properties the alternating copolymer consisting of the above moieties, as indicated by their having viscosity numbers ("I.V.") in the range between 0.6 and 1.5 dl./gm. and TG of 170 DEG to 194 DEG C., with TG vs. I.V. relationship conforming to the formula, TG=192-(11.5/I.V.)+9 and with difference of (TG-HDT) of not over 15 DEG C.; having Izod impact resistance (ft.-lb. per inch of notch) at 25 DEG C. of at least 5; and being essentially free of pyridine and of anhydride linkages. The copolymers preferably have a mol ratio of BPA:TP:carbonate in the range from 2:0.9:1.1 to 2:1.2:0.8, viscosity number of 0.6-1 dl./gm., TG of at least 178 DEG C. by differential scanning calor

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 293.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Bisphenol-A/terephthalate/carbonate copolymer characterized by: (1) being melt processable in the sense that (a) upon compression molding for 10 minutes at 320° C. to form a plaque, said polymer changes in viscosity number by no more than 10% as measured in 40:60 weight ratio of tetrachloroethane:phenol at 25° C. an 0.5 gm./dl. concentration; and (b) when heated under purified nitrogen for 30 minutes at 350° C., then dissolved as a 2% (gm./ml.) solution in dichloromethane, the polymer develops a ∓yellowness index" per ASTM Test No. D:1925, using a 2 cm. path, of no more than 10; (2)

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗