Patents
US 7,270,886 B2#4327040 Most CitedExpiredUnited States (USPTO)Utility

Spin-on glass composition and method of forming silicon oxide layer in semiconductor manufacturing process using the same

20Forward Citations (#4327040 Global)
1.1/yrCitation Velocity (#6111910 Global)
2.34Citation PageRank (#11297325 Global)
15Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A spin-on glass (SOG) composition and a method of forming a silicon oxide layer utilizing the SOG composition are disclosed. The method includes coating on a semiconductor substrate having a surface discontinuity, an SOG composition containing polysilazane having a compound of the formula —(SiH 2 NH) n — wherein n represents a positive integer, a weight average molecular weight within the range of about 3,300 to 3,700 to form a planar SOG layer. The SOG layer is converted to a silicon oxide layer with a planar surface by curing the SOG layer. Also disclosed is a semiconductor device made by the method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 20.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A spin-on glass composition comprising: polysilazane having the compound formula —(SiH2NH) n — wherein n represents a positive integer, in an amount of about 10 to about 30% by weight, based on the total weight of the composition, whereby the polysilazane has a weight average molecular weight within the range of about 3,300 to about 3,700; and a solvent, in an amount of about 70 to about 90% by weight, based on the total weight of the composition, wherein a silicon oxide layer formed using the composition has a reduced number of scratches.

  2. Claim 2Depends on #1

    The spin-on glass composition as claimed in claim 1 , wherein the polysilazane is present in an amount of about 20 to about 23% by weight, based on the total weight of the composition, and the solvent is present in an amount of about 77 to about 80% by weight, based on the total weight of the composition.

  3. Claim 3Independent Claim

    Th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
US 5,310,720 AProcess for fabricating an integrated circuit device by forming a planarized polysilazane layer and oxidizing to form oxide layer199472
JP H08269399 ACoating solution for forming silica-based coating film and substrate having coated film—13
JP H11145286 AManufacture of semiconductor integrated circuit device—23
US 5,976,618 AProcess for forming silicon dioxide film199937
US 2002055271 A1Method of forming silicon oxide layer in semiconductor manufacturing process using spin-on glass composition and isolation method using the same method—30
KR 20020068672 AMethod for forming inter layer dielectric film—10
US 2002160614 A1Method of forming an interlayer dielectric film—18
US 6,479,405 B2Method of forming silicon oxide layer in semiconductor manufacturing process using spin-on glass composition and isolation method using the same method200267
US 2003040194 A1Spin-on glass composition and method of forming silicon oxide layer in semiconductor manufacturing process using the same—15
US 6,566,229 B2Method of forming an insulating layer in a trench isolation type semiconductor device200386
US 6,706,646 B1Spin-on glass composition and method of forming silicon oxide layer in semiconductor manufacturing process using the same200440
US 6,762,126 B2Method of forming an interlayer dielectric film200424
US 7,015,144 B2Compositions including perhydro-polysilazane used in a semiconductor manufacturing process and methods of manufacturing semiconductor devices using the same200614
US 2006094243 A1Compositions including perhydro-polysilazane used in a semiconductor manufacturing process and methods of manufacturing semiconductor devices using the same—9
US 7,053,005 B2Method of forming a silicon oxide layer in a semiconductor manufacturing process200624

Non-Patent Literature (2)

  • Machine translation of JP 08-269399, provided by the JPO website.
  • Office Action dated Nov. 7, 2005 for counterpart Korean application.