Patents
US 7,053,005 B2#3293125 Most CitedExpiredUnited States (USPTO)Utility

Method of forming a silicon oxide layer in a semiconductor manufacturing process

24Forward Citations (#3293125 Global)
1.2/yrCitation Velocity (#5051042 Global)
2.61Citation PageRank (#9486519 Global)
40Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming a silicon oxide layer in a semiconductor manufacturing process includes forming a planar spin on glass (SOG) layer by coating an SOG composition onto a semiconductor substrate having a stepped portion formed thereon, pre-baking the substrate at a temperature of from about 100 to about 500° C. for about 1 to about 10 minutes, maintaining a loading temperature of a furnace into which the substrate will be loaded at about 500° C. or less, loading the substrate into the furnace, and main-baking the substrate at a temperature of from about 500 to about 1200° C. for about 10 to about 120 minutes to form a silicon oxide layer on the substrate. The SOG layer is transformed into the silicon oxide layer through an optimized process condition. Thus, the silicon oxide layer may have minimal defects and a good layer property.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 40 · Forward citations: 24.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a silicon oxide layer in a semiconductor manufacturing process, comprising: forming a planar spin on glass (SOG) layer by coating an SOG composition onto a semiconductor substrate having a stepped portion formed thereon; pre-baking the substrate at a temperature of from about 100 to about 500° C. for about 1 to about 10 minutes; maintaining a loading temperature of a furnace into which the substrate will be loaded at about 500° C. or less; loading the substrate into the furnace; and main-baking the substrate at a temperature of from about 500 to about 1200° C. for about 10

  2. Claim 2Depends on #1

    The method as claimed in claim 1 , further comprising implementing an edge bead removal after forming the SOG layer.

  3. Claim 3Depends on #2

    The method as claimed in claim 2 , further comprising implementi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 24 total)

PatentTitleYearCitations
US 10,647,578 B2N—H free and SI-rich per-hydridopolysilzane compositions, their synthesis, and applications20201
US 8,501,394 B2Superfine-patterned mask, method for production thereof, and method employing the same for forming superfine-pattern20131
US 7,270,886 B2Spin-on glass composition and method of forming silicon oxide layer in semiconductor manufacturing process using the same200720
EP 2,144,279 A2Aminosilanes for shallow trench isolation films—2
US 8,263,717 B2Polysilazane-containing composition capable of forming a dense siliceous film20123
US 2007281498 A1Spin-on glass composition and method of forming silicon oxide layer in semiconductor manufacturing process using the same—6
US 2010234540 A1Polysilazane-containing composition capable of forming a dense siliceous film—9
US 2012296022 A1Polysilazane-containing composition capable of forming a dense siliceous film—1
US 7,582,573 B2Spin-on glass composition and method of forming silicon oxide layer in semiconductor manufacturing process using the same20090
US 2010203299 A1Hardmask Process for Forming a Reverse Tone Image Using Polysilazane—23
US 2015185613 A1Composition for forming a resist underlayer film, and pattern-forming method—16
US 2010040838 A1Hardmask Process for Forming a Reverse Tone Image—41
US 7,999,355 B2Aminosilanes for shallow trench isolation films20115
US 2009104745 A1Integration method for dual doped polysilicon gate profile and cd control—0
US 11,739,220 B2Perhydropolysilazane compositions and methods for forming oxide films using same20231

Non-Patent Literature (2)

  • Machine translation of JP 08-269399, Oct. 1996, Nakajima et al. (obtained from JPO website).
  • Machine translation of JP 09-047722, Feb. 1997, Shibuya et al. (obtained from JPO website).