Patents
US 7,259,055 B2#5842283 Most CitedExpiredUnited States (USPTO)Utility

Method of forming high-luminescence silicon electroluminescence device

16Forward Citations (#5842283 Global)
0.8/yrCitation Velocity (#8647562 Global)
2.57Citation PageRank (#9701570 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for forming a high-luminescence Si electroluminescence (EL) phosphor is provided, with an EL device made from the Si phosphor. The method comprises: depositing a silicon-rich oxide (SRO) film, with Si nanocrystals, having a refractive index in the range of 1.5 to 2.1, and a porosity in the range of 5 to 20%; and, post-annealing the SRO film in an oxygen atmosphere. DC-sputtering or PECVD processes can be used to deposit the SRO film. In one aspect the method further comprises: HF buffered oxide etching (BOE) the SRO film; and, re-oxidizing the SRO film, to form a SiO 2 layer around the Si nanocrystals in the SRO film. In one aspect, the SRO film is re-oxidized by annealing in an oxygen atmosphere. In this manner, a layer of SiO 2 is formed around the Si nanocrystals having a thickness in the range of 1 to 5 nanometers (nm).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for forming a high-luminescence silicon (Si) electroluminescence (EL) phosphor, the method comprising: depositing a silicon-rich oxide (SRO) film having a refractive index in the range of 1.5 to 2.1, and a porosity in the range of 5 to 20%; and post-annealing the SRO film in an oxygen atmosphere to obtain the high-luminance SRO film.

  2. Claim 2Depends on #1

    The method of claim 1 wherein depositing the SRO film includes depositing a SRO film with Si nanocrystals; the method further comprising: following the SRO film post-annealing, hydrofluoric acid (HF) buffered oxide etch (BOE) etching the SRO film; and re-oxidizing the SRO film; and in response to the re-oxidation, Lorning a silicon dioxide (SiO 2 ) layer around the Si nanocrystals in the SRO film.

  3. Claim 3Depends on #2

    The method of claim 2 wherein HF BOE etching the SRO film includes clipping the SRO fil

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Maria E. Castagna et al. "High efficiency light emission devices in silicon." MRS fall meeting, 2002.