Patents
US 6,774,061 B2#1919475 Most CitedExpiredUnited States (USPTO)Utility

Nanocrystalline silicon quantum dots within an oxide layer

33Forward Citations (#1919475 Global)
1.5/yrCitation Velocity (#3396361 Global)
6.55Citation PageRank (#2135510 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process for forming a thin layer of Silicon nanocrystals in an oxide layer is disclosed. The process includes, on a semiconductive substrate, thermally oxidizing a first portion of the substrate into an oxide layer, forming Silicon ions within the layer of oxide, and thermally treating the Silicon ions to become the thin layer of Silicon nanocrystals. In the inventive process the formation of the Silicon ions is by ionic implantation of the Silicon ions into the oxide at an ionization energy of between 0.1 keV and 7 keV, and preferably between 1 and 5 keV. This allows the Silicon atoms to coalesce in a lower temperature than would otherwise be possible. Additionally, more than one layer of nanocrystals can be formed by performing more than one implantation at more than one energy level. Embodiments of the invention can be used to form non-volatile memory devices with a very high quality having a very small size.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 33.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for forming an oxide layer containing a continuous polysilicon layer comprising: forming the oxide layer on a semiconductive substrate; introducing Silicon ions within the oxide layer by ionic implantation of the Silicon ions into the oxide layer at a low energy level under 20 keV and a fluence of about 5×10 16 cm 2 ;and thermally treating the semiconductive substrate at a temperature of between 700 and 800° C. to cause the Silicon ions to become the continuous polysilicon layer.

  2. Claim 2Depends on #1

    The process of claim 1 wherein the oxide layer is thermally grown to a thickness of between 15 and 40 nm prior to being implanted.

  3. Claim 3Depends on #1

    The process of claim 1 wherein the energy level of the ionic implantation is between 0.1 and 7 keV.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Hanafi et al., Fast and Long Retention Time Nanocrystal Memory, Sep. 9, 1996, IEEE, vol. 43, p. 1553-1558.*
  • Normand et al., Formation of 2-D Arrays of Silicon Nanocrystals in Thin SiO2 Films by Very-Low Energy Si Ion Implantation, Feb. 26, 1998, Electorchemical and Solid State Letters, p. 88-90.*
  • Normand, P. et al., "Formation of 2-D Arrays of Silicon Nanocrystals in Thin Sio2 Films by Very-Low Energy Si<+ >Ion Implantation," Electrochemical and Solid State Letters, 1(2):88-90, 1998.
  • Normand, P. et al., “Formation of 2-D Arrays of Silicon Nanocrystals in Thin Sio2 Films by Very-Low Energy Si+ Ion Implantation,” Electrochemical and Solid State Letters, 1(2):88-90, 1998.