Solid state synthesis of lithium ion battery cathode material

42Forward Citations (#1303122 Global)
2.2/yrCitation Velocity (#1685493 Global)
3.71Citation PageRank (#5380126 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Single-phase lithium-transition metal oxide compounds containing cobalt, manganese and nickel can be prepared by wet milling cobalt-, manganese-, nickel- and lithium-containing oxides or oxide precursors to form a finely-divided slurry containing well-distributed cobalt, manganese, nickel and lithium, and heating the slurry to provide a lithium-transition metal oxide compound containing cobalt, manganese and nickel and having a substantially single-phase O3 crystal structure. Wet milling provides significantly shorter milling times than dry milling and appears to promote formation of single-phase lithium-transition metal oxide compounds. The time savings in the wet milling step more than offsets the time that may be required to dry the slurry during the heating step.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 42.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for making single-phase lithium-transition metal oxide compounds containing cobalt, manganese and nickel comprising: a) wet milling cobalt-, manganese-, nickel- and lithium-containing oxides or oxide precursors to form a finely-divided slurry containing well-distributed cobalt, manganese, nickel and lithium, and b) heating the slurry to provide a lithium-transition metal oxide compound containing cobalt, manganese and nickel and having a substantially single-phase O3 crystal structure.

  2. Claim 2Depends on #1

    A process according to claim 1 wherein water is used for wet milling.

  3. Claim 3Depends on #1

    A process according to claim 1 comprising milling the slurry until it contains particles having an average particle diameter less than about 0.3 μm.